Chemical vapor deposition (CVD) diamond is a prospective thin film material for cutting tools applications due to the extreme combination of hardness, chemical inertness, and thermal conductivity. However, the CVD diamond cutting ability of ferrous materials is strongly limited due to its extreme affinity to iron, cobalt, or nickel. The diamond–iron interaction and the diffusion behavior in this system are not well studied and are believed to be similar to the graphite–iron mechanism. In this article, we focus on the medium-temperature working range of 400–800 °C of a CVD diamond–Fe system and show that for these temperatures etching of diamond by Fe is not as strong as is generally accepted. The starting point of the diamond graphitization in contact with iron was found around 400 °C. Our results show that CVD diamond is applicable for the cutting of ferrous materials under medium-temperature conditions.
Results of experiments with the deposition of polycrystalline diamond films onto silicon, titanium, and molybdenum substrates in a specially designed ac glow discharge system are presented. The phase composition and morphology of deposited films have been studied using the atomic force microscopy and X-ray diffraction techniques. It is established that the obtained diamond films possess high purity and degree of crystallinity. Inclusions of non-diamond carbon phases are absent. The rate of diamond film growth in the proposed system is 6–7 μm/h.
1 March 2021 in Instruments and Experimental Techniques
The current state of research and new approaches to solving the problem of heteroepitaxy of diamond films from the gas phase are considered. The features of diamond growth from the gas phase, the nucleation processes, texturing, and the main fundamental problems and barriers of heteroepitaxy of single-crystal diamond are described. Recent achievements and potentially promising approaches in this area are considered.
A combination of two methods of chemical vapor deposition (CVD) of diamond films, microwave plasma–assisted (MW CVD) and hot filament (HF CVD), was used for the growth of 100 µm-thick polycrystalline diamond (PCD) layers on Si substrates. The bow of HF CVD and MW CVD films showed opposite convex\concave trends; thus, the combined material allowed reducing the overall bow by a factor of 2–3. Using MW CVD for the growth of the initial 25 µm-thick PCD layer allowed achieving much higher thermal conductivity of the combined 110 µm-thick film at 210 W/m·K in comparison to 130 W/m·K for the 93 µm-thick pure HF CVD film.