The influence of the ageing temperature on the hardness, electrical conductivity, thermal diffusivity and thermal conductivity of the EN AW-7075 aluminium alloy was studied in this paper. After solution treating the alloy at 480 °C for 1 h and quenching it in ice water, the investigated alloy was characterized using Differential Thermal Analysis (DTA) in order to determine the optimal temperatures for the isochronal ageing treatments. Afterwards, isochronal ageing was conducted at the temperature range of 110 °C-250 °C for 30 min The hardness, electrical conductivity, thermal diffusivity, thermal conductivity and microstructural features were investigated during the ageing treatments. Hardness had a peak value after ageing at 150 °C, while other properties gradually increased with the ageing temperature. Microstructural investigation of the aged alloy by SEM-EDS revealed the existence of precipitated phases that appear homogenously distributed in the microstructure.
The development of reliable lead-free solder alloys remains essential for applications in the electronics industry. This paper investigates the mechanical, electrical, and microstructural properties of a Sn78Bi22 solder alloy. The alloy was prepared by melting and casting, followed by a homogenization heat treatment. Tensile testing, Vickers microhardness measurements, electrical conductivity testing, and SEM/EDS microstructural analysis were performed at room temperature. The investigated alloy exhibited enhanced ultimate tensile strength (~93 MPa) and microhardness (45.5 HV0.05) compared with pure Sn, while electrical conductivity decreased to 5.4 MS/m. These changes were attributed to solid-solution strengthening, grain refinement, and the formation of a Bi-rich secondary phase, which also promoted brittle fracture during tensile testing. Microstructural observations revealed a Sn matrix with finely distributed Bi-rich phases, particularly along grain boundaries. The results contribute additional experimental data on the mechanical, electrical, and microstructural characteristics of non-eutectic Sn-Bi solder alloys.
This paper presents research on the changes in the mechanical and structural properties of the commercial aluminum alloy EN-AW 7075 during thermomechanical processing. The processing involved artificial aging of the alloy at a temperature of 150°C for 30 minutes, followed by cold rolling after aging. Changes in hardness and impact toughness during the experiment were monitored. Hardness was measured using the Leeb method, while impact toughness was measured using the Charpy method. In the annealed state, the lowest hardness values were recorded, while the highest-impact toughness value was achieved in the as-quenched state. By applying cold plastic deformation after artificial aging, the hardness of the alloy significantly increased, while the impact toughness continuously decreased. After deformation of 20%, cracks appearance prevented further deformation. Optical microscopy was used to follow microstructural changes during the applied processing regime. Precipitates of various sizes and morphologies were observed in the structure. The annealed state results in poorly defined grain boundaries and formation of large precipitates relatively evenly distributed throughout the matrix. Cold plastic deformation after aging has resulted in elongated grain structure aligned with the rolling direction, along with crushing of secondary phase particles.
In the present study, the Sn78Bi22 alloy was investigated as a potential solder material. The study focused on the evaluation of thermal diffusivity and thermal conductivity over a defined temperature range, differential scanning calorimetry (DSC) analysis, and an assessment of soldering behavior through measurements of contact angle, spreading area, spreading ratio, and intermetallic compound (IMC) layer thickness. The investigated alloy exhibited reduced thermal diffusivity and thermal conductivity compared with literature data for pure Sn. DSC analysis indicated a decrease in melting temperature compared with pure Sn reported in the literature, resulting from the addition of Bi. Soldering behavior was evaluated as favorable, characterized by a thin IMC layer, a low contact angle on a Cu substrate, and high spreading ratio and spreading area. Based on these results, the Sn78Bi22 alloy shows potential for lead-free soldering applications.