1 January 2018 in Processing and Application of Ceramics
Novel Eu3+-activated M7Sn(PO4)6 (where M = Sr, Ba) red-emitting phosphors were synthesized via conventional solid-state reaction method at 1200 ?C for 2 h. The luminescence properties of the prepared samples and quenching concentration of Sr7-xSn(PO4)6 :xEu3+ and Ba7-xSn(PO4)6 :xEu3+ were investigated. These phosphors can be efficiently excited by UV (395 nm) and visible blue (465 nm) light nicely matching the output wavelengths of the near-UV LEDs and InGaN blue LED chips and emit the red light. The critical concentrations of the Eu3+ activator were found to be 0.175mol and 0.21mol per formula unit for Sr7-xSn(PO4)6 :xEu3+ and Ba7-xSn(PO4)6 :xEu3+, respectively. The M7-xSn(PO4)6 :xEu3+ (M = Sr, Ba) phosphor may be a good candidate for light-emitting diodes application.
13 June 2020 in International Journal of Applied Ceramic Technology
1 January 2021 in Processing and Application of Ceramics
Monoclinic zirconia (ZrO2) whiskers were made via the molten salt method using zirconyl chloride octahydrate (ZrOCl2 ? 8H2O) as zirconium source, potassium chloride (KCl) as molten salt and lithium fluoride (LiF) as a mineraliser. DSC-TG, XRD, FE-SEM, Raman and TEM were performed to study the effects of heat treatment temperature, holding time and heating rate on the synthesis of zirconia whiskers. The results indicate that zirconia whiskers with diameters of 50-80 nm and aspect ratios of 10-30 can be obtained by heating the precursor at slow rate (3?C/min) to 718?C for 1 h and then at faster rate (7?C/min) to 950?C for 3 h. The whiskers have a smooth surface and grow in [001] direction. The key to the ZrO2 whiskers growth is the controlled dissolution and precipitation of the ZrO2 in a LiF-KCl molten salt solution environment.
1 January 2018 in Processing and Application of Ceramics
ZrO2 whiskers have been synthesized by a facile molten salt method using ZrOCl2 ? 8H2O and Na3PO4 ? 12H2O as the zirconium source and molten salt, respectively. Differential thermal and thermogravimetric analyses, Xray diffraction analysis, field emission scanning electron microscope and transmission electron microscope were employed to characterize the heating process of the precursor mixture, phase composition of the assynthesized ZrO2 whiskers and the effect of reaction temperature on the synthesis of ZrO2 whiskers. The results show that the ZrO2 whiskers synthesized at 900?C have an average aspect ratio of 30 and preferentially grow along [010] direction. The formation of sodium zirconium phosphate [Na9-4xZrx(PO4)3] (x = 1, 2) and the reaction temperature play an important role in the growth of ZrO2 whiskers. This work also suggests an effective route for mass production of high quality ZrO2 whiskers.
12 January 2023 in Journal of Materials Science: Materials in Electronics