School of Integrated Circuit Science and Engineering, State Key Laboratory of Crystal Materials, Engineering Research Center of Optoelectronic Devices and Communication Technology, Tianjin University of Technology 1 , Tianjin 300384
Auto-generated profile, based on publicly available information
Yan Zhu
School of Integrated Circuit Science and Engineering, State Key Laboratory of Crystal Materials, Engineering Research Center of Optoelectronic Devices and Communication Technology, Tianjin University of Technology 1 , Tianjin 300384
In this study, we explored the fabrication, structural characteristics, and optical properties of Zn2GeO4 thin films grown on c-cut Al2O3 substrates via radio frequency magnetron sputtering. The crystalline quality, surface morphology, and optical characteristics were comprehensively evaluated at various annealing temperatures, and the 700 °C-annealed film presented the best crystallization quality. XRD and TEM results revealed the microstructure of Zn2GeO4 film and confirmed that the epitaxial relationship is Zn2GeO4 (0006)//Al2O3 (0006) with Zn2GeO4 [11¯00]//Al2O3 [11¯00]. O 1s spectrum indicated the bandgap of the 700 °C-annealed film is 4.98 eV. UV-Vis-Near Infrared spectroscopy showed that the average transmittance reached approximately 85% in the visible region, and the optical bandgap of Zn2GeO4 film annealed at 700 °C was about 5.02 eV.
This work reports the zirconium-doped indium oxide (IZRO) transparent conductive thin films on infrared optical quartz glass (JGS-3) substrates via room-temperature RF magnetron sputtering. The effects of annealing temperature and oxygen flow ratio on electrical and optical properties were systematically investigated. The optimized IZRO film with 3 sccm oxygen flow and 700 °C annealing temperatures exhibited an average optical transmittance of 91.5% in the wavelength of 1300–1550 nm and a minimum resistivity of 1.37 × 10−3 Ω·cm with a carrier concentration of 2.46 × 1020 cm−3. The results of x-ray photoelectron spectroscopy revealed that the enhanced electrical conductivity can be attributed to the activation of Zr doping through high-temperature annealing. Meanwhile, the structural and morphological properties of the obtained films were investigated in detail. The IZRO films have potential in the field of short-wave infrared (SWIR) optoelectronic devices due to their SWIR transparent conductive properties.
8 April 2026 in Materials Science in Semiconductor Processing
This paper proposes two wavelength-extended InGaAs p-type semiconductor - intrinsic absorption layer - n-type semiconductor structures to achieve methane detection at low temperatures. The responsivity of the strained and metamorphic structures is 0.98 and 1.09 A/W at 20 °C. The strained structure detector can achieve a response level of 0.7 A/W in low-temperature environments above −10 °C. The metamorphic structure shows a responsivity not less than 0.8 A/W within the temperature span of −40 to 85 °C. The dark current of both devices is at the nA level at −10 V. The saturation optical power of the strained structure and the metamorphic structure is 13 and 17 mW at −0.5 V, respectively. The cut-off wavelength is 1690 and 1730 nm for the strained structure and the metamorphic structure. These two structures tested by x-ray diffraction have high crystalline quality. The strained structure has a root mean square roughness of 0.13 nm, while the metamorphic structure's roughness is 0.39 nm. These results suggest that both strained and metamorphic structures have promising applications in low-temperature probes.
The attractive properties of zinc germanate (Zn2GeO4), including a wide bandgap and high chemical stability, make it promising for ultraviolet (UV) photodetection. However, the impact of its crystallization state on device performance remains underexplored. In this work, metal-semiconductor-metal (MSM)-structured photodetectors were fabricated based on amorphous and crystalline willemite-type Zn2GeO4 thin films. The crystalline detector exhibited superior temporal response: under 8 V bias and 235 nm illumination, its rise time and decay time were 1.14 s and 44 ms, respectively, significantly faster than those of the amorphous counterpart (4.92 s and >10 s). The crystalline device also showed lower dark current (8.2 pA vs. 98.7 nA) and better wavelength selectivity in the UV-C range. These improvements are attributed to reduced defect density and enhanced carrier transport in the crystalline phase. This study demonstrates that crystallization engineering is an effective strategy for optimizing the performance of Zn2GeO4-based UV photodetectors.