Emad El-Kashif

Emad El-Kashif

Auto-generated profile, based on publicly available information

Emad El-Kashif

Department of Mechanical Design and Production, Faculty of Engineering, Cairo University, Giza, Egypt

Research Focus & Metrics

Academic Career Length

13Years (2014-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 January 2021 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
Sherif MehannySherif Mehanny
Sherif Mehanny
EMEhab E. Abu-El Magd
Ehab E. Abu-El Magd
MIMaha Ibrahim
Maha Ibrahim
MFMahmoud Farag
Mahmoud Farag
RGRodrigo Gil-San-Millan
Rodrigo Gil-San-Millan
EEEmad El-Kashif
Emad El-Kashif

7 June 2023 in Heliyon
Verified
Journal Article
Open access
ARAbdallah Refate
Abdallah Refate
YMYehia Mohamed
Yehia Mohamed
MMMariam Mohamed
Mariam Mohamed
MSMaiada Sobhy
Maiada Sobhy
KSKarim Samhy
Karim Samhy
Sherif MehannySherif Mehanny
Sherif Mehanny
Electrospinning is an effective method for producing high-quality biopolymer nanofibers, such as cellulose and chitosan. Cellulose nanofibers have excellent mechanical properties and biocompatibility, making them a promising material for tissue engineering. Chitosan nanofibers are biodegradable, biocompatible, and antimicrobial, making them ideal for biomedical applications. The electrospinning parameters, including solution concentration, power supply voltage, orifice diameter, temperature, humidity, and flow rate, play a crucial role in determining the nanofiber diameter, morphology, and mechanical properties, as well as their suitability for various applications. This systematic review aims to synthesize and evaluate the current evidence on the influence of electrospinning parameters on the production and properties of cellulose and chitosan nanofibers. A comprehensive search of electronic databases was conducted to identify relevant studies. The inclusion criteria were studies that investigated the effect of electrospinning parameters on cellulose and chitosan nanofibers. It was found that for cellulose, the average fiber diameter increased with increasing each of solution concentration, power supply voltage, orifice diameter, temperature, and humidity. Contrary to tip - collector distance and some optimal points in temperature, where average fiber diameter decreased. For chitosan, the change in voltage and tip to collector distance did not alter the average fiber diameter except for some readings of voltage, which behaved differently. On the other hand, the average fiber diameter increased with increasing flow rate. The review highlights the importance of considering electrospinning parameters in the production of high-quality biopolymer nanofibers and provides insights into the optimization of these parameters for specific applications. This review also highlights the need for further research to better understand the underlying mechanisms of electrospinning and to optimize the process to produce biopolymer nanofibers with improved properties.

13 February 2023 in Metals
Verified
Journal Article
Open access
PDF file
Mahmoud A. EssamMahmoud A. Essam
Mahmoud A. Essam
Ahmed Yehia ShashAhmed Yehia Shash
Ahmed Yehia Shash
MEMohamed Kamal El-Fawakhry
Mohamed Kamal El-Fawakhry
EEEmad El-Kashif
Emad El-Kashif
HMHassan Megahed
Hassan Megahed
Shock resisting cold work tool steel is one of the most applicable steels for several applications such as cutting sheets, chisels, hammers, etc. It has been categorized according to its characteristic properties into different categories as hot and cold work tool steel. This work aims to study the effects of conventional and deep cryogenic treatment (DCT) on shock-resistant cold work tool steel. In this study, three alloys were cast and prepared with different carbides forming elements such as vanadium (V) and niobium (Nb). The samples were quenched in water at 900 ℃ followed by a tempering treatment at 200 ℃  for 30 min. After quenching in water, the other samples were subjected to DCT at −196 ℃  for a 5-h soaking time, followed by tempering at 200 ℃  for 30 min. To study the wear behavior of the three heats, pin-on-disc tests were used, where the sliding speed was kept constant at a value of 0.5 m/s. The normal applied loads during the wear test were 50 N and 100 N. In order to understand the wear behavior, wear tracks were studied by scanning electron microscopy, coefficient of friction and weight loss were evaluated. The results showed that the lowest average coefficient of friction was achieved by a sample of steel 3 with quenching + DCT at a load of 100 N of load by value of 0.33. A sample of steel 3 at load 50 N achieved the lowest weight loss by using DCT plus tempering. On the other hand, a sample of steel 3 achieved the lowest weight loss at 100 N by using quenching + DCT.

1 January 2021 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
AEAbou Bakr Elshalakany
Abou Bakr Elshalakany
VTVineet Tirth
Vineet Tirth
EEEmad El-Kashif
Emad El-Kashif
HHHussein Mohammed Abdel Moneam Hussein
Hussein Mohammed Abdel Moneam Hussein
WHW. Hoziefa
W. Hoziefa

26 April 2014 in Welding in the World
Verified
Journal Article
Closed access
PDF file
MMM. Morsy
M. Morsy
EEE. El-Kashif
E. El-Kashif

1 January 2014 in Zavarivanje i zavarene konstrukcije
Verified
Journal Article
Closed access
PDF file
MMM. Morsy
M. Morsy
EEE. El-Kashif
E. El-Kashif
Surface modification of mild steel was under-taken using two covered electrodes and two tubular electrodes. The two covered electrodes are DIN 8555: E6-UM-60 and E10-UM-60GR; however, the two tubular electrodes are E10-GF-60GR1 and E10-GF-60GR2. Chemical analysis for the weld metal and XRD of the flux covering for covered electrodes and flux core for tubular electrodes were conducted. The most important factor in determining the wear resistance is the microstructure of the deposit layers. In similar carbon equivalent electrodes E10-UM-60GR and E10-GF-60GR1, electrode E10-GF-60GR1 (tubular) shows larger carbides area fraction and better wear resistance than electrode E10-UM-60GR (covered). This could be attributed to a lower dilution associated with tubular electrode compared with covered electrode. The two tubular electrodes showed higher wear resistance than the covered electrodes which is mainly due to the larger Fe-Cr carbide precipitation area fraction.