1 September 2021 in Acta Biomaterialia
The increased risk of fracture in the elderly associated with metabolic conditions like osteoporosis poses a significant strain on health care systems worldwide. Due to bone's hierarchical nature, it is necessary to study its mechanical properties and failure mechanisms at several length scales. We conducted micropillar compression experiments on ovine cortical bone to assess the anisotropic mechanical response at the lamellar scale over a wide range of strain rates (10-4 to 8·102 s-1). At the microscale, lamellar bone exhibits a strain rate sensitivity similar to what is reported at the macroscale suggesting that it is an intrinsic property of the extracellular matrix. Significant shear band thickening was observed at high strain rates by HRSEM and STEM imaging. This is likely caused by the material's inability to accommodate the imposed deformation by propagation of thin kink bands and shear cracks at high strain rates, leading to shear band thickening and nucleation. The post-yield behavior is strain rate and direction dependent: hardening was observed for transverse oriented micropillars and hardening modulus increases with strain rate by a factor of almost 2, while axially oriented micropillars showed strain softening and an increase of the softening peak width and work to ultimate stress as a function of strain rate. This suggests that for compression at the micrometer scale, energy absorption in bone increases with strain rate. This study highlights the importance of investigating bone strength and post-yield behavior at lower length scales, under hydrated conditions and at clinically relevant strain rates. STATEMENT OF SIGNIFICANCE: We performed micropillar compression experiments of ovine cortical bone at two different orientations and over seven orders of magnitude of strain rate. Experiments were performed under humid condition to mimic the natural conditions of bone in a human body using a newly developed micro-indenter setup. The strain rate sensitivity was found to be of a similar magnitude to what has been reported for higher length scales, suggesting that the strain rate sensitivity is an intrinsic property of the bone extracellular matrix. In addition, localized shear deformation in thick bands was observed for the first time at high strain rates, highlighting the importance of investigating bone under conditions representative of an accident or fall at several length scales.
30 November 2022 in Small
1 August 2022 in Journal of the Mechanical Behavior of Biomedical Materials
Preclinical studies often require animal models for in vivo experiments. Particularly in dental research, pig species are extensively used due to their anatomical similarity to humans. However, there is a considerable knowledge gap on the multiscale morphological and mechanical properties of the miniature pigs' jawbones, which is crucial for implant studies and a direct comparison to human tissue. In the present work, we demonstrate a multimodal framework to assess the jawbone quantity and quality for a minipig animal model that could be further extended to humans. Three minipig genotypes, commonly used in dental research, were examined: Yucatan, Göttingen, and Sinclair. Three animals per genotype were tested. Cortical bone samples were extracted from the premolar region of the mandible, opposite to the teeth growth. Global morphological, compositional, and mechanical properties were assessed using micro-computed tomography (micro-CT) together with Raman spectroscopy and nanoindentation measurements, averaged over the sample area. Local mineral-mechanical relationships were investigated with the site-matched Raman spectroscopy and micropillar compression tests. For this, a novel femtosecond laser ablation protocol was developed, allowing high-throughput micropillar fabrication and testing without exposure to high vacuum. At the global averaged sample level, bone relative mineralization demonstrated a significant difference between the genotypes, which was not observed from the complementary micro-CT measurements. Moreover, bone hardness measured by nanoindentation showed a positive trend with the relative mineralization. For all genotypes, significant differences between the relative mineralization and elastic properties were more pronounced within the osteonal regions of cortical bone. Site-matched micropillar compression and Raman spectroscopy highlighted the differences between the genotypes' yield stress and mineral to matrix ratios. The methods used at the global level (averaged over sample area) could be potentially correlated to the medical tools used to assess jawbone toughness and morphology in clinics. On the other hand, the local analysis methods can be applied to quantify compressive bone mechanical properties and their relationship to bone mineralization.
22 February 2023 in ACS Applied Nano Materials
13 April 2023 in Acta Biomaterialia
The hierarchical design of bio-based nanostructured materials such as bone enables them to combine unique structure-mechanical properties. As one of its main components, water plays an important role in bone's material multiscale mechanical interplay. However, its influence has not been quantified at the length-scale of a mineralised collagen fibre. Here, we couple in situ micropillar compression, and simultaneous synchrotron small angle X-ray scattering (SAXS) and X-ray diffraction (XRD) with a statistical constitutive model. Since the synchrotron data contain statistical information on the nanostructure, we establish a direct connection between experiment and model to identify the rehydrated elasto-plastic micro- and nanomechanical fibre behaviour. Rehydration led to a decrease of 65%-75% in fibre yield stress and compressive strength, and 70% in stiffness with a 3x higher effect on stresses than strains. While in agreement with bone extracellular matrix, the decrease is 1.5-3x higher compared to micro-indentation and macro-compression. Hydration influences mineral more than fibril strain with the highest difference to the macroscale when comparing mineral and tissue levels. The effect of hydration seems to be strongly mediated by ultrastructural interfaces while results provide insights towards mechanical consequences of reported water-mediated structuring of bone apatite. The missing reinforcing capacity of surrounding tissue for an excised fibril array is more pronounced in wet than dry conditions, mainly related to fibril swelling. Differences leading to higher compressive strength between mineralised tissues seem not to depend on rehydration while the lack of kink bands supports the role of water as an elastic embedding influencing energy-absorption mechanisms. STATEMENT OF SIGNIFICANCE: Characterising structure-property-function relationships in hierarchical biological materials helps us to elucidate mechanisms that enable their unique properties. Experimental and computational methods can advance our understanding of their complex behaviour with the potential to inform bio-inspired material development. In this study, we close a gap for bone's fundamental mechanical building block at micro- and nanometre length scales. We establish a direct connection between experiments and simulations by coupling in situ synchrotron tests with a statistical model and quantify the behaviour of rehydrated single mineralised collagen fibres. Results suggest a high influence of hydration on structural interfaces, and the role of water as an elastic embedding by outlining important differences between wet and dry elasto-plastic properties of mineral nanocrystals, fibrils and fibres.
29 September 2025 in Advanced Engineering Materials
Two‐photon polymerization (2PP) is an additive manufacturing technology capable of producing polymeric 3D nano‐ to mesoscale structures with design flexibility and sub‐micron resolution. This study investigates the influence of 2PP printing parameters on the morphology and mechanical properties of solid and porous microstructures fabricated from three commercial resins: IP‐Q, IP‐S, and IP‐polydimethylsiloxane (IP‐PDMS). To evaluate micromechanical behavior, micropillar compression tests are conducted using IP‐Q, which has not been extensively characterized. Porous structures retained 80–85% of the stiffness of solids for IP‐Q and IP‐S, and 50% for IP‐PDMS. Fourier transform infrared spectroscopy showed degrees of conversion of 38% for IP‐Q and 61% for IP‐S and IP‐PDMS. The optimal printing parameters for IP‐Q micropillars were a laser power of 50 mW, slicing distance (s) of 1.2 μm, and hatching distance (h) of 1 μm. These settings correspond to a peak laser intensity of 1.58 × 10 −11 W cm −2 , a focal spot diameter (dxy) of 3.17 μm, a Rayleigh length (zR) of 10.13 μm, and a voxel overlap (δ) of 0.6. These conditions yielded a Young's modulus of 3.7 GPa and yield strength of 75.21 MPa. Overall, the findings emphasize the challenges of parameter optimization when introducing porosity and comparing materials. The results provide a systematic framework for tailoring 2PP processing to guide biomedical microdevice design.