AB2Sb2-type Zintl phases, particularly Mg3Sb2-based materials, have recently garnered significant attention owing to their earth-abundant, nontoxic constituents and excellent n-type thermoelectric (TE) performance in the medium temperature range. However, achieving high-performance all Mg3Sb2-based TE devices remains difficult due to the lack of a compatible and efficient p-type counterpart. Herein, a combined approach of Cu doping and Yb alloying is employed to synergistically optimize the carrier concentration, carrier mobility, and reduce lattice thermal conductivity, thereby achieving a high-performance p-type Mg3Sb2 TE material. Consequently, a high zT value of 0.95 is obtained for the optimized composition Mg1.18Cu0.02Zn1.2Yb0.6Sb2 at 673 K. To demonstrate practical applicability, a fully compatible Mg3Sb2-based TE device is fabricated using cupronickel as a common diffusion barrier for both p- and n-type legs, ensuring excellent interfacial stability and device reliability. A crack-free interface with a specific contact resistivity of ρc ∼ 2.76 μΩcm2 is achieved. The single-leg p-type device exhibited a maximum efficiency, ηmax ∼ 5.5%, while for a two-pair TE device, ηmax ∼ 9.2% at a temperature difference (ΔT) of 374 K is realized. These findings demonstrate the potential of compositional engineering for developing efficient p-type Mg3Sb2 materials and fully integrated TE devices for waste heat recovery.
SrCuSb-based Zintl compounds are promising midtemperature thermoelectric materials but suffer from high lattice thermal conductivity and suboptimal charge transport. In this work, a codoping approach is implemented by substituting aliovalent In and isovalent Bi for Sb in SrCuSb, thereby simultaneously tuning carrier transport and enhancing phonon scattering. Polycrystalline SrCuSb1–x–yInxBiy (0 ≤ x ≤ 0.125, y = 0, 0.05, 0.07), synthesized by melting, ball milling, and spark plasma sintering, shows that In adjusts the hole concentration and preserves high mobility. At the same time, Bi introduces mass/strain-field disorder that softens the lattice and thereby suppresses lattice thermal conductivity. Codoping also suppresses the formation of secondary phases, improving phase purity and carrier mobility. The optimized SrCuSb0.825In0.125Bi0.05 composition exhibits a high power factor of ∼1.9 mW/m·K2 and a low lattice thermal conductivity of ∼0.52 W/m·K at 773 K, yielding a peak zT of ∼0.65. The average zT over 300–773 K increases from 0.17 for pristine SrCuSb to 0.32, corresponding to an ∼87% enhancement. These results demonstrate that aliovalent–isovalent codoping is an effective and widely applicable route to simultaneously engineer carrier transport and phonon scattering, advancing midtemperature thermoelectric materials based on planar Zintl phases.
18 September 2025 in Science and Technology of Advanced Materials
The pursuit of sustainable thermoelectric materials requires the development of cost-effective and efficient compounds derived from earth-abundant elements. Here, we investigate the effects of samarium (Sm) substitution on the thermoelectric performance of SrSi₂ with compositions Sr1-xSmxSi2 (x = 0, 0.05, 0.1, 0.15, and 0.2). Substituting Sm for Sr in SrSi₂ enhances the power factor at low substitution levels, while further substitution leads to a decrease, due to increased carrier scattering and reduced Seebeck coefficient. Introducing Sm substitution enhances phonon scattering through point defects, reducing lattice thermal conductivity. A peak figure of merit (ZT) of ~0.23 at room temperature is achieved for Sr₀.₉₅Sm₀.₀₅Si₂, demonstrating a 35% improvement over undoped SrSi₂. The weighted mobility of ~285 cm2/V·s and the tailored thermal transport emphasize the role of Sm substitution in modulating both electronic and thermal properties. These findings establish Sr1-xSmxSi2 as a promising candidate for next-generation thermoelectric devices.
14 October 2026 in Journal of Alloys and Compounds