31 October 2023 in Journal of Welding and Joining
Solidification cracking during lithium-ion battery packaging was metallurgically investigated, specifically for Cu-steel dissimilar materials. To this end, single-mode fiber and green lasers were employed under heat input conditions ranging from 1.3 to 8.0 J/mm. For both laser welds, solidification cracking was concentrated in the steel region of the fusion zone, particularly in the locally Cu-depleted region, regardless of the welding condition. Modified self-restraint tests were performed for overlapping dissimilar material combinations to elucidate the mechanism of solidification cracking. Analysis of the solidification cracking surface revealed that approximately 15?30 mass% Cu existed on the surface. Cu was highly enriched with a droplet shape, formed during solidification within the miscibility gap. By calculating the non-equilibrium weld mushy zone range based on the diffusion-controlled Scheil’s model, the solidification cracking in the Cu-depleted region was estimated at 453 K. It was strongly affected by the severe segregation of Cu (95.7 mass%) in the residual liquid at the terminal stage of the solidification path. Therefore, from a welding metallurgical perspective, homogeneous Cu distribution and minimization of Cu segregation within the fusion zone are essential for suppressing or minimizing the solidification cracking susceptibility of Cu?steel dissimilar laser welding.
30 April 2025 in Journal of Welding and Joining
This study analyzed the microstructure and mechanical properties of arc-welded joints in XM-19 stainless steel using type 312 welding materials. For GTAW, ER312 welding materials were used, while E312 covered electrode were applied in SMAW. The mechanical properties of the welded joints were evaluated through tensile and impact testing, and discussed in relation to microstructure analysis results. The welds with type 312 welding materials met the allowable tensile strength requirement but did not surpass the allowable impact absorption energy threshold. The low impact absorption energy observed in the welds with type 312 welding consumables is attributed to the brittleness induced by the high delta ferrite content, as well as the significant presence of hot cracking in the welds. Although these hot cracks did not significantly affect the tensile strength, they are believed to have contributed to rapid crack propagation under localized stress during the impact test, leading to a sharp reduction in impact absorption energy. This study provides valuable insights into the effects of type 312 welding materials and welding process on the mechanical properties and microstructure of welded joints in XM-19 stainless steel.