The pulsed laser welding of Al ribbon to Cu sheet was investigated for the electrical interconnections in power electronic modules. The various experimental conditions with the different laser powers, scan speeds, and heat inputs were employed for obtaining the defect-free Al/Cu joints. During the Al/Cu laser welding, the intermetallic compounds were formed in the welding zone. An electron probe microanalyzer and transmission electron microscopy confirmed the phases of intermetallic compounds, which were found to be Al4Cu9, Al2Cu, AlCu, etc. The computational fluid dynamics simulation revealed that the Marangoni effect induced the circulation of the molten pool, resulting in the mixture of Al and Cu and the formation of swirl-like structures at the Al/Cu joints. The tensile shear strengths and electrical resistances of the Al/Cu joints were measured, and they showed a strong correlation with the welding area. A decrease in mechanical strength and an increase in electrical resistance were measured with increasing the welding area of Al/Cu joints. Moreover, the process window for the defect-free Al/Cu joints was developed, and the experimental conditions for Al/Cu laser braze-welding were examined to minimize the intermetallic compounds formation at the Al/Cu joints.
In modern high-intensity ultrafast laser processing, detecting the focal position of the working laser beam, at which the intensity is the highest and the beam diameter is the lowest, and immediately locating the target sample at that point are challenging tasks. A system that allows in-situ real-time focus determination and fabrication using a high-power laser has been in high demand among both engineers and scientists. Conventional techniques require the complicated mathematical theory of wave optics, employing interference as well as diffraction phenomena to detect the focal position; however, these methods are ineffective and expensive for industrial application. Moreover, these techniques could not perform detection and fabrication simultaneously. In this paper, we propose an optical design capable of detecting the focal point and fabricating complex patterns on a planar sample surface simultaneously. In-situ real-time focus detection is performed using a bandpass filter, which only allows for the detection of laser transmission. The technique enables rapid, non-destructive, and precise detection of the focal point. Furthermore, it is sufficiently simple for application in both science and industry for mass production, and it is expected to contribute to the next generation of laser equipment, which can be used to fabricate micro-patterns with high complexity.
Precise and rapid focus detection is an essential operation in several manufacturing processes employing high-intensity lasers. However, the detection resolution of existing methods is notably low. This paper proposes a technique that provides a rapid-response, high-precision, and high-resolution focus inspection system on the basis of geometrical optics and advanced optical instruments. An ultrafast interface position detector and a single-slit mask are used in the system to precisely signal the focus position with high resolution. The reflected images on the image sensor are of a high quality, and this quality is maintained persistently when the target surface is shifted along the optical axis. The proposed system developed for focus inspection is simple and inexpensive, and is appropriate for practical use in the industrial production of sophisticated structures such as microcircuits and microchips.
Solidification cracking during lithium-ion battery packaging was metallurgically investigated, specifically for Cu-steel dissimilar materials. To this end, single-mode fiber and green lasers were employed under heat input conditions ranging from 1.3 to 8.0 J/mm. For both laser welds, solidification cracking was concentrated in the steel region of the fusion zone, particularly in the locally Cu-depleted region, regardless of the welding condition. Modified self-restraint tests were performed for overlapping dissimilar material combinations to elucidate the mechanism of solidification cracking. Analysis of the solidification cracking surface revealed that approximately 15?30 mass% Cu existed on the surface. Cu was highly enriched with a droplet shape, formed during solidification within the miscibility gap. By calculating the non-equilibrium weld mushy zone range based on the diffusion-controlled Scheil’s model, the solidification cracking in the Cu-depleted region was estimated at 453 K. It was strongly affected by the severe segregation of Cu (95.7 mass%) in the residual liquid at the terminal stage of the solidification path. Therefore, from a welding metallurgical perspective, homogeneous Cu distribution and minimization of Cu segregation within the fusion zone are essential for suppressing or minimizing the solidification cracking susceptibility of Cu?steel dissimilar laser welding.
28 February 2024 in Journal of Welding and Joining
This study investigates a green laser welding on a nickel-coated copper-mild steel material used in an electric vehicle battery. The laser power and scan speed were varied, and through optical microscopy, it was demonstrated that excessive heat input led to increased weld penetration depth and bead width. Regarding defects, excessive heat input caused the formation of oxide, spatter on the bead surface, as well as porosity and cracks inside the weld penetration depth. The mechanical properties were evaluated through shear stress and microhardness measurements, indicating that as the heat input increased, the mechanical properties improved for the sample welded under the 2 kW condition. Considering the fire risk (occur at weld penetration depth over 50%) and joining aspects (start at weld penetration depth higher 20%), the optimal conditions were set as 1.6 kW and 300 mm/s. This optimized condition was set as the reference for monitoring. Based on the optimized condition, the results shown that an increase in heat input led to increased plasma and temperature signals, and an increase in scanning speed resulted in an increase in reflected light signal.
This paper describes the development of a welding profile sensor for the laser welding robot application. The sensor consists of a PC based vision camera and a stripe-type laser diode. All components are assembled into a compact module which can be attached to the end-effector of welding robots. The laser-stripe sensor can measure the profile of the welding object and obtain the seam line. Moreover, the working distance of the sensor can be varied. The robot, the seam tracking system, and CW Nd:YAG laser are used for the laser welding robot system. The simple control scheme of the whole system is also presented. The profile measurement and the seam tracking experiments were carried out to validate the operation of the system.