In this work, the piezoresistive effects of defective graphene used on a flexible pressure sensor are demonstrated. The graphene used was deposited at substrate temperatures of 750, 850 and 1000 °C using the hot-filament thermal chemical vapor deposition method in which the resultant graphene had different defect densities. Incorporation of the graphene as the sensing materials in sensor device showed that a linear variation in the resistance change with the applied gas pressure was obtained in the range of 0 to 50 kPa. The deposition temperature of the graphene deposited on copper foil using this technique was shown to be capable of tuning the sensitivity of the flexible graphene-based pressure sensor. We found that the sensor performance is strongly dominated by the defect density in the graphene, where graphene with the highest defect density deposited at 750 °C exhibited an almost four-fold sensitivity as compared to that deposited at 1000 °C. This effect is believed to have been contributed by the scattering of charge carriers in the graphene networks through various forms such as from the defects in the graphene lattice itself, tunneling between graphene islands and tunneling between defect-like structures.
A bimetallic cobalt‐iron catalyst was utilized to demonstrate the growth of multiwalled carbon nanotubes (CNTs) at low gas pressure through thermal chemical vapor deposition. The characteristics of multiwalled CNTs were investigated based on the effects of catalyst thickness and gas pressure variation. The results revealed that the average diameter of nanotubes increased with increasing catalyst thickness, which can be correlated to the increase in particle size. The growth rate of the nanotubes also increased significantly by ~2.5 times with further increment of gas pressure from 0.5 Torr to 1.0 Torr. Rapid growth rate of nanotubes was observed at a catalyst thickness of 6 nm, but it decreased with the increase in catalyst thickness. The higher composition of 50% cobalt in the cobalt‐iron catalyst showed improvement in the growth rate of nanotubes and the quality of nanotube structures compared with that of 20% cobalt. For the electrical properties, the measured sheet resistance decreased with the increase in the height of nanotubes because of higher growth rate. This behavior is likely due to the larger contact area of nanotubes, which improved electron hopping from one localized tube to another.