19 April 2023 in Journal of Vacuum Science & Technology B
The wide bandgap semiconductors SiC and GaN are commercialized for power electronics and for visible to UV light-emitting diodes in the case of the GaN/InGaN/AlGaN materials system. For power electronics applications, SiC MOSFETs (metal–oxide–semiconductor field effect transistors) and rectifiers and GaN/AlGaN HEMTs and vertical rectifiers provide more efficient switching at high-power levels than do Si devices and are now being used in electric vehicles and their charging infrastructure. These devices also have applications in more electric aircraft and space missions where high temperatures and extreme environments are involved. In this review, their inherent radiation hardness, defined as the tolerance to total doses, is compared to Si devices. This is higher for the wide bandgap semiconductors, due in part to their larger threshold energies for creating defects (atomic bond strength) and more importantly due to their high rates of defect recombination. However, it is now increasingly recognized that heavy-ion-induced catastrophic single-event burnout in SiC and GaN power devices commonly occurs at voltages ∼50% of the rated values. The onset of ion-induced leakage occurs above critical power dissipation within the epitaxial regions at high linear energy transfer rates and high applied biases. The amount of power dissipated along the ion track determines the extent of the leakage current degradation. The net result is the carriers produced along the ion track undergo impact ionization and thermal runaway. Light-emitting devices do not suffer from this mechanism since they are forward-biased. Strain has also recently been identified as a parameter that affects radiation susceptibility of the wide bandgap devices.
26 April 2024 in Journal of Vacuum Science & Technology B
High-power electronics, such as GaN high electron mobility transistors (HEMTs), are expected to perform reliably in high-temperature conditions. This study aims to gain an understanding of the microscopic origin of both material and device vulnerabilities to high temperatures by real-time monitoring of the onset of structural degradation under varying temperature conditions. This is achieved by operating GaN HEMT devices in situ inside a transmission electron microscope (TEM). Electron-transparent specimens are prepared from a bulk device and heated up to 800 °C. High-resolution TEM (HRTEM), scanning TEM (STEM), energy-dispersive x-ray spectroscopy (EDS), and geometric phase analysis (GPA) are performed to evaluate crystal quality, material diffusion, and strain propagation in the sample before and after heating. Gate contact area reduction is visible from 470 °C accompanied by Ni/Au intermixing near the gate/AlGaN interface. Elevated temperatures induce significant out-of-plane lattice expansion at the SiNx/GaN/AlGaN interface, as revealed by geometry-phase GPA strain maps, while in-plane strains remain relatively consistent. Exposure to temperatures exceeding 500 °C leads to almost two orders of magnitude increase in leakage current in bulk devices in this study, which complements the results from our TEM experiment. The findings of this study offer real-time visual insights into identifying the initial location of degradation and highlight the impact of temperature on the bulk device’s structure, electrical properties, and material degradation.
15 May 2023 in Applied Physics Letters
In this work, we demonstrate the rejuvenation of Ti/4H-SiC Schottky barrier diodes after forward current-induced degradation, at room temperature and in a few seconds, by exploiting the physics of high-energy electron interactions with defects. The diodes were intentionally degraded to a 42% decrease in forward current and a 9% increase in leakage current through accelerated electrical stressing. The key feature of our proposed rejuvenation process is very high current density electrical pulsing with low frequency and duty cycle to suppress any temperature rise. The primary stimulus is, therefore, the electron wind force, which is derived from the loss of the momentum of the high energy electrons upon collision with the defects. Such defect-specific or “just in location” mobilization of atoms allows a significant decrease in defect concentration, which is not possible with conventional thermal annealing that requires higher temperatures and longer times. We show evidence of rejuvenation with additional improvement in leakage current (16%) and forward current (38%) beyond the pristine condition. Transmission electron microscopy, geometric phase analysis, Raman spectroscopy, and energy dispersive x-ray-spectroscopy reveal the enhancement of defects and interfaces. The ultrafast and room temperature process has the potential for rejuvenating electronic devices operating in high power and harsh environmental conditions.