A large density difference of a basin-type insulator in gas-insulated metal-enclosed switchgear (GIS) weakens its mechanical strength, which will threaten the safe and stable operation of GIS. In this article, an ultrasonic nondestructive testing method for density uniformity of GIS basin-type insulators was proposed. First, seven standard samples with different Al 2 O 3 content were tested by an ultrasonic testing system, and then a mapping relationship between density and ultrasonic velocity was established. Second, the uncertainty of the testing system was obtained, and the ultrasonic velocities of 192 positions in a 126 kV three-phase basin-type insulator were measured. Finally, the density distribution of the insulator was obtained based on the mapping equation of velocity-density, and a contour plot of density was established by the cubic spline interpolation. The results show that there was a positive linear correlation between the density of standard samples and the ultrasonic velocity, and the determination coefficient was 0.992. Notably, the expanded uncertainty of ultrasonic propagation time for detecting 45 mm-thick EP/Al 2 O 3 composites was only 0.0112 μs. The ultrasonic propagation time of detection positions in the insulator was from 31.0634 to 31.4708 μs and the difference was greater than 0.0112 μs, which illustrated that the testing system meets the requirements for detecting the density of the insulator. According to the contour plot of density, the density distribution of the insulator was shown clearly and efficiently. The density was higher at the bottom edge of the insulator and the upper part of the insert, whereas the density was smaller at the lateral upper part of the insulator and the lower part of the insert. Specifically, the maximum density of the insulator was 2.36 g/cm 3 and the minimum density was 2.25 g/cm 3 . The feasibility of nondestructive testing density by the ultrasonic method is verified, which provides a new method for density evaluation of GIS insulators.
22 December 2021 in IEEE Transactions on Instrumentation and Measurement
Thermal stress of gas-insulated metal-enclosed switchgear (GIS) basin-type insulators weaken its mechanical properties, which will threaten the safe and stable operation of GIS. In this article, the simulation and experiment of thermal stress in a 252-kV GIS basin-type insulator were carried out. An acoustic-distance difference method based on the ultrasonic critical refraction longitudinal wave (ultrasonic $L_{\mathrm {CR}}$ ) and a measuring method for propagation depth of ultrasonic $L_{\mathrm {CR}}$ were proposed respectively: the variation of propagation depth in epoxy composites was measured by ultrasonic probes of different frequencies, and a mapping function between the propagation depth and detection frequency was established. The 2-MHz variable-angle ultrasonic probes were used to test the circumferential thermal stress below the surface of the 252-kV basin-type insulator, and the thermal stress simulation of the insulator was performed. The circumferential thermal stress at different positions of the insulator was obtained and then a contour plot of the stress was established by the cubic spline interpolation. The results showed that the propagation depth of ultrasonic $L_{\mathrm {CR}}$ in the subsurface of epoxy composites decreased exponentially with the frequency, the mapping relationship of depth-frequency had a good goodness of fit, and the coefficient of determination was as high as 0.988. The circumferential thermal stress at 9 mm below the surface of the insulator was tensile stress, which decreased first and then increased along the radial direction, showing as a V-shaped distribution. The experimental values were in good agreement with the simulation values, which verified the effectiveness of the proposed methods.
25 January 2021 in IEEE Transactions on Instrumentation and Measurement
The multifactor accelerated aging test is an important means to predict the lifetime of gas-insulated switchgear (GIS) O-ring seals, while the leakage rate (LR) is a potential index for failure evaluation. This article proposed a three-factor accelerated aging test platform and a leakage test system (LTS) for GIS seal rings. The aging factors are thermal, mechanical compression, and pressured SF 6 gas. The pressure aging vessel (PAV) can be filled with various gases to simulate the operating conditions of the GIS and age multiple samples simultaneously. During the aging process, leakage tests are conducted on flange pairs without disassembling and separating the seal rings. After the test, the aging can be continued so as to study the evolution of LR with aging time. In order to analyze the properties of leakage test and validate the platform, a three-factor accelerated aging and a traditional two-factor accelerated aging (thermal and compression) were conducted on GIS O-ring seals of EPDM material. Compression set (CS) and LR were tested. The result showed that a steady inherent LR F 0 exists for the LTS. The LR rose linearly with accumulating time, allowing simplified calculation of LR. The three-factor aged samples had significantly smaller CS than those of the two-factor aged samples, indicating that the working condition of GIS with SF 6 atmosphere significantly slows the aging rate of GIS seal rings. The findings proved that the three-factor accelerated aging test platform and LTS effectively simulate the operating conditions of GIS seal rings and evaluate their properties.
In recent years, decay-like fracture has become the main fracture form of composite insulators, and the faults caused by it seriously threaten the safety and stability of the power system. In this paper, decay-like fracture composite insulators string on the 500kV are used as samples to determine the physical and chemical properties of their shed. Its physical properties are detected by appearance inspection, hardness, pollution test and hydrophobicity; its chemical properties are detected by nuclear magnetic resonance and Fourier transform infrared spectroscopy. The physical and chemical characteristics of the decay-like fracture shed are obtained, it is found that decay is closely related to aging and partial discharge is also an important factor leading to the decay of composite insulators.
1 January 2026 in IEEE Transactions on Dielectrics and Electrical Insulation