The aim of this study was to evaluate the microhardness and surface roughness of composite resins immersed in alcoholic beverages. Three composite resins were used: Durafill (Heraeus Kulzer), Z250 (3M-ESPE) and Z350 XT (3M-ESPE). The inital surface roughness and microhardness were measured. The samples were divided into four groups (n=30): G1-artificial saliva; G2-beer; G3-vodka; G4-whisky. The samples were immersed in the beverages 3× a day for 15 min and 30 days. The surface roughness and microhardness assays were repeated after immersion period. The data were statistically analyzed by two-way ANOVA and Tukey-HSD test (p<0.05). Surface roughness increased for all composite resins immersed in beer and whisky. Microhardness of all groups decreased after immersion in alcoholic beverages. The effect of these beverages on dental composites is depended upon the chemical composition, immersion time, alcohol content and pH of solutions.
The aim of this study was to evaluate the effect of different glass fiber posts (GFPs) diameters on the push-out bond strength to dentin. Forty unirradicular human teeth were endodontically treated and used for cementation of GFPs (White Post DC, FGM) with different diameters (n=10): P1 - ø 1.6 mm coronal x 0.85 mm apical; P2 - ø 1.8 mm coronal x 1.05 mm apical; P5 - ø 1.4 mm coronal x 0.65 mm apical; and PC - customized post number 0.5 with composite resin (Tetric Ceram A2, Ivoclair Vivadent). All GFPs were cemented into the root canal using a dual-curing luting composite (Variolink II, Ivoclar Vivadent). One slice (1.7 mm) of each root third of cemented GFP (cervical, middle, and apical) was submitted to push-out testing. Failure modes of all specimens were classified as: adhesive failure between resin cement and post; adhesive failure between dentin and resin cement; cohesive failure within resin cement, post or dentin; and mixed failure. The data were analyzed with two-way ANOVA and Tukey’s test (a=0.05). The highest bond strength values were presented for the P2 and PC groups. There was no statistically significant difference between the GFP thirds in each group. The groups P2, P5, and PC showed predominantly adhesive failure. For P1, the most prevalent type of failure was adhesive between resin cement and post. It may be concluded that a glass fiber post that is well adapted to the root canal presents higher bond strength values, regardless of GFP third.
1 November 2017 in Materials Science and Engineering: C