14 August 2018 in Advanced Healthcare Materials
31 May 2021 in Advanced Optical Materials
Phase‐change materials (PCMs) and phase‐transition materials (PTMs) both show a large contrast in their respective optical properties upon switching, enabling compact optical components with diverse functionalities like sensing, thermal imaging, and data recording. However, their switching properties differ significantly, that is, the switching is non‐volatile for PCMs while volatile for PTMs. Here, new‐generation smart mid‐infrared modulators with switchable transmission, reflection, and absorption are demonstrated conceptually and experimentally, which combine one PCM (Ge3Sb2Te6 or In3SbTe2) with one PTM (VO2) as two active layers. The bottom VO2 layer is employed as a thermally regulated (modulated) dynamic mirror, facilitating the switching of transmission between “on” state (using VO2 in its semiconducting state at temperatures below its phase transition temperature Tc) and “off” state (metallic VO2 at temperatures above Tc). The PCM layer on top of the metallic VO2 layer is used either for continuously adjusting the absorption peak spectrally (by up to 1.8 µm using different phases of Ge3Sb2Te6) or for switching between absorption mode (A = 0.99 with amorphous In3SbTe2) and reflection mode (R = 0.85 with crystalline In3SbTe2). The presented concept of merging static, non‐volatile thermal switching (via PCMs) with dynamic, volatile thermal modulation (via PTMs) empowers a new generation of optical devices for smart optical switching, for example in spectrally tunable safety optical switches.
30 April 2020 in CrystEngComm
The crystal structure and second-harmonic generation response of the new nonlinear optical material, Sr4Pb1.5Sb5O5Se8, were examined.
24 September 2015 in Journal of Vacuum Science & Technology A
A VO2 film exposed to ambient air is prone to oxidation, which will degrade its thermochromic properties. In this work, the authors deposited an ultrathin Al2O3 film with atomic layer deposition (ALD) to protect the underlying VO2 film from degradation, and then studied the morphology and crystalline structure of the films. To assess the protectiveness of the Al2O3 capping layer, the authors performed a heating test and a damp heating test. An ultrathin 5-nm-thick ALD Al2O3 film was sufficient to protect the underlying VO2 film heated at 350 °C. However, in a humid environment at prolonged durations, a thicker ALD Al2O3 film (15 nm) was required to protect the VO2. The authors also deposited and studied a TiO2/Al2O3 bilayer, which significantly improved the protectiveness of the Al2O3 film in a humid environment.
1 February 2008 in Journal of Non-Crystalline Solids