Herein, we report the structural evolution and the rich sequence of magnetic transitions in GdMn1–xFexO3 (x = 0, 0.3, and 0.5) synthesized through the sol-gel technique. Rietveld refinement of X-ray diffraction patterns reveals a structural transformation from O′ to O type orthorhombic one accompanied with a decrease in lattice volume when x increases from 0 to 0.5. The decrease in lattice volume is due to the presence of Mn4+ confirmed from X-ray photoelectron spectroscopy and photoluminescence (PL) studies. Such a structural transformation considerably reduces the Jahn-Teller distortion factor as indicated by Raman and PL spectra. The temperature dependent magnetization shows an increase in Néel temperature (TN) from ∼42 K for pristine GdMnO3 to almost room temperature for x = 0.5. Interestingly, we observe a spin reorientation temperature (TSR) at ∼270 and ∼253 K for x = 0.3 and 0.5, respectively. The mixed valency of Mn, i.e., Mn3+ and Mn4+ not only demonstrates a spin-glass (SG) behavior but also contributes toward the strong emission spectra irrespective of Fe concentration. The structural and magnetic properties of GdMnO3 after doping Fe suggest a possible way to achieve a better magnetoelectric coupling and modify the multiferroic property.
Bulk hafnium oxide (HfO2) exhibits the monoclinic phase at room temperature which transforms to tetragonal and cubic phases at 1700 and 2600 °C, respectively, under ambient conditions. For the first time, we observe a monoclinic to stable cubic phase transformation at room temperature in nanoparticles of HfO2 by incorporating Sm3+ ions up to 12 at. %. Although the monoclinic structure is retained at 1 at. % of Sm, a mixed phase of monoclinic and cubic is observed at intermediate Sm concentration (5–11 at. %). Le-Bail profile refinement of X-ray diffraction patterns confirms the monoclinic to cubic phase transformation with increasing Sm3+ ion concentration. While the significant difference in ionic radii of Sm3+ and Hf4+ ion induces strain in the lattice above 9 at. %, a lower valency of Sm produces oxygen vacancy leading to 8-fold coordination with Sm3+ ion and stabilizes the cubic phase at room temperature. Not only the particle size obtained from transmission electron micrograph (TEM) matches well with the size calculated from the Williamson-Hall plot, the lattice spacing estimated from high resolution TEM also confirms the monoclinic and cubic phases in HfO2 and Hf0.88Sm0.12O2, respectively. Apart from phase transformation induced by Sm3+ ions, photoluminescence studies demonstrate an excellent emission in near green and red regions in Hf1−xSmxO2 nanoparticles. A schematic energy band diagram has been proposed based on the excitation and emission processes involved in HfO2 and Hf0.99Sm0.01O2 nanoparticles.
6 February 2024 in Materials Chemistry and Physics