Solvolysis of elastane in blended fabrics using tert -amyl alcohol and KOH (cat.) provides elastane monomers and a fibre matrix. The process is especially useful for polyamide/elastane blends, providing a possibility for fibre-to-fibre recycling.
12 February 2025 in Beilstein Journal of Nanotechnology
Polymeric membranes offer an appealing solution for sustainable CO2 capture, with potential for large-scale deployment. However, balancing high permeability and selectivity is an inherent challenge for pristine membranes. To address this challenge, the development of mixed matrix membranes (MMMs) is a promising strategy. MMMs are obtained by carefully integrating porous nano-fillers into polymeric matrices, enabling the simultaneous enhancement of selectivity and permeability. In particular, metal-organic frameworks (MOFs) have gained recognition as MMM fillers for CO2 capture. Here, a review of the current state, recent advancements, and challenges in the fabrication and engineering of MMMs with MOFs for selective CO2 capture is proposed. Key considerations and promising research directions to fully exploit the gas separation potential of MOF-based MMMs in CO2 capture applications are highlighted.
5 January 2024 in Journal of Material Cycles and Waste Management
The push for increasing the recycling of plastics is intensifying, and the growing use of composites creates a need to increase the recyclability of polymer composites at their end-of-life. As opposed to thermal and chemical recycling techniques, recycling by dissolution has the benefit of enabling the recovery of both fibre and matrix from thermoplastic composites without altering their chemical composition. In this study, suspensions of polypropylene and glass fibres of varying concentrations were obtained upon dissolution in xylene heated to 130 °C. Subsequent filtration enabled the separation and recovery of both clean fibre and polypropylene fractions. The chemical structures of both fractions were identified by Fourier transformed infrared spectroscopy as pure polypropylene and clean glass fibres. The recovered glass fibres contained 1 wt% organic material from glass fibre sizing, and the recovered and pristine polypropylene showed no sign of remaining fibres.