Conductive hydrogels are becoming one of the most important milestones for the development of new scaffolds, biosensors, supercapacitors, and green electronics within the field of biomedicine. In this work, we study the effect of different types of electroactive additives such as poly(3,4-ethylenedioxythiophene), tannic acid, and carbon quantum dots (CQDs), to form different poly(vinyl alcohol) (PVA)-based hydrogels with enhanced electrochemical properties. Different physicochemical tests are carried out to characterize the different PVA-based hybrid hydrogels and the rates of their degradation and loss of electroactivity throughout an eight-week biodegradation process. This work shows the individual and synergistic effects of the additives on various mechanical properties, including storage modulus and swelling ratio, and electrochemical properties of the PVA hydrogel. The additives have proven to enhance the electroactivity of the PVA-based hydrogels but as well their degradation. Finally, the use of the new hydrogel as a pressure sensor is also investigated. The study provides an insight on the potential use of CQDs, in synergy with other electroactivity enhancers, in the fabrication of novel hybrid conducting hydrogels in green electronics. Graphical Abstract
The stability of duplex stainless steel (DSS) laser‐surface textured (LST) in brine solutions is of significant interest for industrial applications. The present study reports evidences that passive films on smooth DSS2205 surfaces (Blank) deteriorate early (96 h). This lower performance is detected in anodic polarization and in accelerated cyclic polarization tests with increasing exposition time and in harsh conditions. Although both surfaces maintain their chemical resistance against corrosion in noncyclic potentiodynamic experiments, the LST microstructure shows a broader passivation area with a larger potential range than the control samples. Moreover, the DSS2205 microstructure patterned surface is preserved. On the contrary, localized corrosion with macroscopic pits and microcracks is extended on the whole Blank surface. The α / γ crystalline phase ratio was reduced in corroded flat surface, while it remains stable in the corroded LST specimens, thanks to a significant formation of FeCr 2 O 4 as a protective oxide film, as proved by Raman. Thus, LST treatments promise some advantages over nontreated interfaces, particularly for metallic pieces that will be in contact or installed close to salt environments.