Thick-shell InP/ZnSe III–V/II–VI quantum dots (QDs) were synthesized with two distinct interfaces between the InP core and ZnSe shell: alloy and core/shell. Despite sharing similar optical properties in the spectral domain, these two QD systems have differing amounts of indium incorporation in the shell as determined by high-resolution energy-dispersive x-ray spectroscopy scanning transmission electron microscopy. Ultrafast fluorescence upconversion spectroscopy was used to probe the charge carrier dynamics of these two systems and shows substantial charge carrier trapping in both systems that prevents radiative recombination and reduces the photoluminescence quantum yield. The alloy and core/shell QDs show slight differences in the extent of charge carrier localization with more extensive trapping observed in the alloy nanocrystals. Despite the ability to grow a thick shell, structural defects caused by III–V/II–VI charge carrier imbalances still need to be mitigated to further improve InP QDs.
The incorporation of quantum dots in display technology has fueled a renewed interest in InP-based quantum dots, but difficulty controlling the Zn chemistry during shelling has stymied thick, even ZnSe shell growth. The characteristic uneven, lobed morphology of Zn-based shells is difficult to assess qualitatively and measure through traditional methods. Here, we present a methodological study utilizing quantitative morphological analysis of InP/ZnSe quantum dots to analyze the impact of key shelling parameters on InP core passivation and shell epitaxy. We compare conventional hand-drawn measurements with an open-source semi-automated protocol to showcase the improved precision and speed of this method. Additionally, we find that quantitative morphological assessment can discern morphological trends in morphologies that qualitative methods cannot. In conjunction with ensemble fluorescence measurements, we find that changes to shelling parameters that promote even shell growth often do so at the cost of core homogeneity. These results indicate that the chemistry of passivating the core and promoting shell growth must be balanced carefully to maximize brightness while maintaining emission color-purity.