21 September 2018 in AIP Conference Proceedings
Leachate wastewater from pulp and paper industry is known for containing various types of heavy metals such as Cd (Cadmium), Ba (Barium) and Cu (Cuprum). The existence of heavy metals that accumulates and eventually exceeds certain threshold concentrations will cause environmental pollution, therefore it is necessary to conduct wastewater treatment to eliminate or at least reduce the heavy metal content in industrial wastewater. One of the most commonly used wastewater treatment method is using adsorbent, this study uses adsorbent made from the mixture of clay, zeolite and activated carbon formed into ceramic balls with ± 0.5 cm diameter. The ratios of the mixture of clay, zeolite and activated carbon are 6:3:1; 6:2,5:1,5; 6:2:2; 6:1,5:2,5 and 6:1:3 with variations of contact time 30, 60, 90, 120 and 150 minutes. The most favorable concentration reduction of heavy metals occurred at the longest contact time of 150 minutes at 6:3:1 adsorbent ratio, Cd concentration decreases from 0.65 mg/L to 0.03 mg /L, Ba concentration decreases from 0.86 mg/L to 0.04 mg/L and Cu concentration is from 0.6 mg/L to 0.02 mg/L. These prove that the ceramic zeolite/carbon-ceramic composite adsorbent can be an alternative to treat wastewater containing heavy metals derived from the pulp and paper industry.
1 January 2017 in AIP Conference Proceedings
Increasing textile industries in Indonesia resulted in increasing the utilization of dyes. The use of synthetic dyes are still dominating because they have many advantages. But, synthetic dyes are difficult to decompose in nature so they can cause potential pollution if discharged directly into the environment. In this study, Procion Red was used as a model of synthetic dye wastewater. The objective of this research is to study the effect of TiO2 catalyst concentration and irradiation time on the degradation of Procion Red under solar irradiation. Photo degradation takes place by using TiO2 catalyst powder in the various concentration of Procion Red of 150-300 ppm. The various concentrations of TiO2 catalyst of 0.5-8 g/l were used. The color and COD degradation of Procion Red for 12 hours of solar irradiation were investigated. Color degradation was measured by using a spectrophotometer. While COD degradation was measured by using Ferrous Ammonium Sulfate (FAS) analysis method. The result showed when using Procion Red of 150 ppm, the highest color degradation of 100% was achieved by using TiO2 catalyst of 6 g/l and the highest COD degradation of 62% was obtained by using TiO2 catalyst of 8 g/l, under 12 hours of solar irradiation
21 September 2018 in AIP Conference Proceedings
The widespread use of plastic in the citizen’s life could cause environmental problems. Plastic is synthesis polymer made from the petroleum product which is difficult to decompose naturally in nature. This study reprocess expanded polystyrene and multilayer as raw materials using pyrolysis in fixed bed reactor into fuel oil. The ratios of the raw material of expanded polystyrene and multilayer plastic are 1:0, 9:1, 4:1, 7:3, 3:2, 1:1, 2:3, 3:7, 1:4, 1:9, 0:1 with the raw material mass is 250 gram. The cracking time is 30 minutes and 60 minutes at the temperature cracking of 250°C. This research reveals that the physical properties of the product which are density, viscosity, heat value, and flash point through GC-MS analysis results were aromatic compound. The highest result is the styrene compound at ratio (1: 1) is 44.34%, at ratio (0: 1) is 40.59% and at ratio (1: 0) is 28.56%. The addition of multilayer plastics is able to increase the percentage of styrene but also decrease the percentage of other benzene, that is ethylbenzene.
1 February 2023 in Open Ceramics
1 September 2019 in IOP Conference Series: Materials Science and Engineering
Paper making requires raw materials with high cellulose and hemicellulose content. The alternative materials that can be used in the paper making are sugarcane bagasse and banana midrib. The paper production method used in this study is acetosolve which involves acetic acid as an organic solvent. The objectives of this research are to figure out the acetic acid concentration in delignification process and the ratio between sugarcane bagasse and banana midrib that produce pulp with the highest yield, cellulose and kappa number. In this research, there are some variables, the first is the levels of acetic acid concentration in delignification process, which are 70%, 75%, 80%, 85%, 90%, the second is the ratio between sugarcane bagasse and banana midrib, which are 20:0, 18:2, 16:4, 14:6, 12:8, 10:10. The results show that the best pulping conditions are found to be 80% acetic acid concentration with 12:8 (w/w) ratio between sugarcane bagasse and banana midrib, and also 1:20 (w/v) ratio between raw material and solution of acetic acid at two hours cooking duration. The highest yield of pulp in acetosolve process was 63.1%, and its characteristics are 84.67% of cellulose and 10.44 kappa number.