School of Materials Science and Engineering & National Key Laboratory for Precision Hot Processing of Metals, Harbin Institute of Technology, Harbin 150001, China
Auto-generated profile, based on publicly available information
Xunmao Zhong
School of Materials Science and Engineering & National Key Laboratory for Precision Hot Processing of Metals, Harbin Institute of Technology, Harbin 150001, China
The isothermal compression experiment of as-rolled Ti55 alloy was carried out on a Gleeble-3800 thermal simulation test machine at the deformation temperature range of 700–1050 °C and strain rate range of 0.001–1 s−1. The hot deformation behavior and the microstructure evolution were analyzed during thermal compression. The results show that the apparent activation energy Q in α+β dual-phase region and β single-phase region were calculated to be 453.00 KJ/mol and 279.88 KJ/mol, respectively. The deformation softening mechanism was mainly controlled by dynamic recrystallization of α phase and dynamic recovery of β phase. Discontinuous yielding behavior mainly occurred in β phase region, which weakened gradually with the increase of deformation temperature (>990 °C) and strain rate (0.01–1 s−1) in β phase region. The processing map derived from Murty’s criterion was more accurate in predicting the hot workability than that derived from Prasad’s criterion. The optimized hot working window was 850–975°C/0.001–1 s−1, in which sufficient dynamic recrystallization occurred and α + β-transus microstructure was obtained. When deformed at higher temperature (≥1000 °C), coarsened lath-shape β-transus microstructure was formed, while deformed at lower temperature (≤825 °C) and higher strain rate (≥0.1 s−1), the dynamic recrystallization was not sufficient, thus flow instability appeared because of shear cracking.
In order to study the effect of initial microstructures on the hot deformation behavior and workability of Ti2AlNb alloy, the isothermal compression experiments of as-rolled and solution-treated Ti–19Al–23Nb–0.5Mo alloys were conducted in the temperature range of 900–1100 °C and strain rate range of 0.001–10 s−1. Subsequently, the processing maps of different state materials were established based on dynamic material model (DMM) and Prasad’s instability criterion. The suitable regions for hot working were determined in the processing maps, which was verified through high-temperature tensile test. The results show that although the solution-treatment could be used to improve the ductility of as-rolled Ti2AlNb alloy at room temperature, the as-rolled microstructure exhibited better hot workability at high temperature compared to the solution-treated microstructure.