24 November 2014 in Applied Physics Letters
Uniformly distributed and defect-free vertically aligned ZnO nanorods (NRs) with high aspect ratio are deposited on Si by sputtering technique. X-ray diffraction along with transmission electron microscopy studies confirmed the single crystalline wurtzite structure of ZnO. Absence of wide band emission in photoluminescence spectra showed defect-free growth of ZnO NRs which was further conformed by diamagnetic behavior of the NRs. H2 sensing mechanism based on the change in physical dimension of channel is proposed to explain the fast response (∼21.6 s) and recovery times (∼27 s) of ZnO NRs/Si/ZnO NRs sensors. Proposed H2 sensor operates at low temperature (∼70 °C) unlike the existing high temperature (>150 °C) sensors.
20 July 2015 in Journal of Applied Physics
Vertically well aligned ZnO nanorods (NRs) were grown on Si(100) substrate using RF magnetron sputtering technique. Scanning electron microscopy images confirms uniform distribution of NRs on 2 in. wafer with average diameter, height and density being ∼75 nm, ∼850 nm, and ∼1.5 × 1010 cm−2, respectively. X-ray diffraction reveals that the ZnO NRs are grown along c-axis direction with wurtzite crystal structure. Cathodoluminescence spectroscopy, which shows a single strong peak around 3.24 eV with full width half maxima 130 meV, indicates the high crystalline and optical quality of ZnO and very low defect density. Vertically aligned nanosensors were fabricated by depositing gold circular Schottky contacts on ZnO NRs. Resistance responses of nanosensors were observed in the range from 50 to 150 °C in 1% and 5% hydrogen in argon environment, which is below and above the explosive limit (4%) of hydrogen in air. The nanosensor's sensitivity increases from 11% to 67% with temperature from 50 to 150 °C and also shows fast response time (9–16 s) and moderate recovery time (100–200 s). A sensing mechanism is proposed based on Schottky barrier changes at heterojunctions and change in depletion region of NRs.
1 June 2015 in AIP Advances
ZnO thick Stress relaxed films were deposited by reactive magnetron sputtering on 2”-wafer of SiO2/Si at room temperature. The residual stress of ZnO films was measured by measuring the curvature of wafer using laser scanning method and found in the range of 0.18 x 109 to 11.28 x 109 dyne/cm2 with compressive in nature. Sputter pressure changes the deposition rates, which strongly affects the residual stress and surface morphologies of ZnO films. The crystalline wurtzite structure of ZnO films were confirmed by X-ray diffraction and a shift in (0002) diffraction peak of ZnO towards lower 2θ angle was observed with increasing the compressive stress in the films. The band gap of ZnO films shows a red shift from ∼3.275 eV to ∼3.23 eV as compressive stress is increased, unlike the stress for III-nitride materials. A relationship between stress and band gap of ZnO was derived and proposed. The stress-free growth of piezoelectric films is very important for functional devices applications.
14 July 2023 in Optics & Laser Technology
SMSourangshu Mukhopadhyay