8 November 2023 in Superconductivity
Verified
Journal Article
Open access
XLX.Q. Lai
X.Q. Lai
JZJ.X. Zuo
J.X. Zuo
XHX.B. Hu
X.B. Hu
TZT. Zhang
T. Zhang
JLJ.D. Liu
J.D. Liu
PLP.Y. Li
P.Y. Li

22 February 2024 in IEEE Transactions on Applied Superconductivity
Verified
Journal Article
Closed access
XLX. Q. Lai
X. Q. Lai
JZJ. X. Zuo
J. X. Zuo
XHX. B. Hu
X. B. Hu
PLP. Y. Li
P. Y. Li
Cables in large-scale fusion magnets are subjected to high transverse electromagnetic forces caused by high currents and magnetic fields. Consequently, they require sufficient mechanical strength to ensure safe and stable operation. To meet this requirement, a high-temperature superconducting (HTS) cable-in-conduit conductor (CICC) suitable for fusion reactors has been manufactured. Each conductor contains 10 round strands, and each strand is composed of a stack of 20 tapes (2 mm wide) surrounded by filling material (Sn 63 Pb 37 ) and a copper former. The conductor is further encased in a round stainless steel jacket to accommodate the large Lorentz forces. To investigate the degradation of the critical current ( Ic ) under cyclic transverse loads, two prototype conductors, each approximately 1.4 m long, were fabricated using REBCO coated conductor tapes. Both conductors have the Ic around 8.8 kA in self-field at 77 K. Additionally, cyclic transverse loading tests were performed at 77 K, self-field. The results revealed that the conductors were able to withstand large transverse loads (>200 MPa) with less than 5% degradation of the Ic . However, a significant reduction in the Ic (∼25%) was observed after 100 cycles, with the load amplitudes ranging from 20 MPa to 200 MPa. When the conductor was subjected to 500 to 10,000 cycles, no significant change in the Ic was observed at ∼65% of its original value. Finally, to further understand and enhance the Ic characteristics of the conductor, we investigated the defects caused by fabrication imperfections and mechanical loading microscopically. Our results will have significant implications for further improving the mechanical strength of the conductor and its application in fusion magnets.

29 July 2024 in IEEE Transactions on Applied Superconductivity
Verified
Journal Article
Closed access
RWRun Wu
Run Wu
XHXinbo Hu
Xinbo Hu
XLXiaoqiang Lai
Xiaoqiang Lai
LCLijun Cai
Lijun Cai
Bending stresses in winding magnets cause the degradation of the performance of HTS conductors. Here, we tested the critical currents ( Ic ) of a Bi2223 stacked-tape cable under bending and analyzed the stress distribution and the Ic of the cable under bending by finite elements method (FEM). Then we analyzed the Ic of the stacked-tape CICC conductor under bending. The experimental results show that the critical bending radius ( rc ) of the cable is about 0.25 m, which is similar to the results of FEM. The rc of the CICC conductor is about 2.4 m and the 4-slots CICC conductor has the smallest rc at the bending angle of 45°.