Alperen Oz

Alperen Oz

Auto-generated profile, based on publicly available information

Alperen Oz

Hacettepe University

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
27 September 2021 in Clinical and Experimental Health Sciences
Verified
Journal Article
Closed access
CACansu Atalay
Cansu Atalay
AOAlperen Oz
Alperen Oz
MIMirna Abou Ibrahi̇m
Mirna Abou Ibrahi̇m
MSMoath Shaqar
Moath Shaqar
MTMarah Tayyem
Marah Tayyem
GGGüliz Nigar Guncu
Güliz Nigar Guncu
Aim: To assess the effect of three different polishing protocols on the surface roughness and color change of the enamel and compare the results with the enamel specimens exposed to coffee. Methods: Seventy-two bovine enamel specimens were randomly divided into two groups-Group I:only polishing,Group II:immersion in coffee solution and polishing–which were then subdivided into 3 groups according to polishing procedures as follows:polishing with rubber cup and Pumice Flour(PF),polishing with rubber cup and Prophy Paste(PP),polishing with Air Abrasion(AA). Surface roughness(Ra) and tooth color were assessed using a surface profilometer and a digital spectrophotometer. The color change was determined by the CIE L*a*b* system. SEM analysis were also performed. Statistical analyses were performed by GraphPad software. Multiple comparisons between-groups and in-groups were performed using Kruskal-Wallis and Friedman tests, respectively. Results: At baseline measurements, no significant differences were found among groups in terms of roughness and color values(p>0.05). In Group I,surface roughness values and color change were similar after polishing (p:0.393,p:0.093, respectively). In Group II,post-polishing Ra values were significantly increased in all groups(p0.05) and the highest ΔE value was detected in PP group. Conclusion: Following coffee immersion, enamel surfaces become rougher in all polishing protocols and the roughest surface was in PF group. In all study groups visible clinical success was achieved in terms of color, therefore dental clinicians should prefer PP in clinical practice due to the less abrasive and sufficient color change properties.

23 December 2024 in Selcuk Dental Journal
Verified
Journal Article
Open access
EMEce Meral
Ece Meral
MPMeltem Nermin Polan
Meltem Nermin Polan
AOAlperen Oz
Alperen Oz
EEEsra Ergin
Esra Ergin
Background: The aim of this study was to assess the microshear bond strength(μSBS) of various adhesive systems on enamel surfaces prepared using either an Er, Cr:YSGG laser or a conventional diamond bur. Methods: Twenty-eight caries-free human molars were longitudinally sectioned, resulting in 56 samples. Buccal or lingual surfaces were embedded in acrylic blocks. Enamel surfaces were prepared using either an Er, Cr: YSGG laser (Biolase Technologies, USA) or a traditional diamond bur (Diatech, Switzerland), referencing the midline of each tooth. Laser treatment was applied to the left side, while the right half underwent bur treatment. The samples were randomly separated into four groups(n=14): [G1] Optibond FL (Kerr, USA), a three-step etch-and-rinse adhesive; [G2] Clearfil SE Bond(Kuraray,Japan), a two-step self-etch adhesive; [G3]Prime&Bond Universal(Dentsply,USA),universal-adhesive/etch-and-rinse-mode; and [G4]Prime&Bond Universal(Dentsply,USA),universal-adhesive/self-etch-mode. Composite cylinders with a diameter of 0.8 mm (Harmonize, Kerr, USA) were affixed to the center of both the laser-prepared and bur-prepared regions of all specimens. The adhesive interface of one randomly chosen representative from each group was analyzed using a Scanning Electron Microscope(SEM). The remaining samples were subjected to μSBS testing. Data were analyzed statistically using Two-Way ANOVA(p0.05). Regardless of the preparation modalities, the adhesive systems did not exhibit any statistically significant differences(p>0.05). Furthermore, the correlation between various adhesive systems and preparation techniques did not result in statistically significant variations in μSBS values(p>0.05). Conclusion: The measured μSBS values of the adhesive systems examined on enamel surfaces prepared using either an Er, Cr:YSGG laser or a diamond bur showed similarity. Keywords: Laser preparation, Microshear bond strength, Scanning electron microscopy, Universal adhesive.