The development of batteries with new materials typically starts with small active material amounts and consequently with small cells, often with low-loaded electrodes. As development progresses to increasing technology readiness levels, mid-sized and large cells with thicker electrode coatings are mandatory. However, large cells have different electrochemical and physicochemical properties than small lab cells. Herein, we discuss similarities and especially differences in the behavior of small laboratory cells (e.g. coin) and larger cells (cylindrical, pouch, prismatic), regarding cell design, electrode thickness, specific energy on material and cell level, heating behavior due to current flow, impedance, voltage curves, and rate capability. Impedances at 1 kHz are reduced by three orders of magnitude from coin cells to large cells while heating power is increased by a factor of 10 2 to 10 5 . By comparing specific capacities on cathode material level with those on cell level for commercial cells, we find a reduction by a factor of ∼3 to ∼5, depending on the anode coating thickness. The large general gap from pure material to cell and between small laboratory, mid-sized, large pilot, and commercial cells need to be taken into account from the beginning of battery development to avoid potential misinterpretation.
1 September 2025 in Journal of the Electrochemical Society
In contrast to conventional graphite electrodes, silicon-graphite electrodes allow a considerable increase in specific energy and energy density of lithium-ion batteries. Nevertheless, the degradation of silicon-rich slurries during rest times in production before electrode coating remains a central challenge for direct implementation of such electrodes on an industrial scale. In this study, the degradation of five slurry variations with different Si contents is investigated with a focus on rheological changes, the quantification of temperature dependent gas formation and its impact on cycle life in battery full cells. Our results show that H2 is formed as a reaction product between the electrochemically active silicon component and water that is used as a solvent in the coating process. Gas volume measurements and mass spectrometry are used to determine the extent of H2 gas formation from different slurry formulations and under different storage conditions. In addition, electrochemical tests with 40 coin full cells show that changes during slurry storage and with the associated silicon oxidation impairs cell cyclability. Our study provides insights into the mechanisms of slurry degradation for silicon-graphite electrodes and identifies strategies to mitigate H2 formation, which improves the cycle life of high-energy lithium-ion battery cells.
Storage of electrode slurries between mixing and coating can affect electrode quality and subsequent cell performance. Here, water-based silicon/graphite anode slurries with five Si/C composite-to-graphite ratios were stored for up to 14 d under continuous stirring at room temperature (RT) or statically at 5 °C and compared with previously reported static RT storage. Rheology, zeta potential, maximum particle size, and electrochemical performance were evaluated. All slurries remained shear-thinning, but viscosity decreased during storage. Continuous stirring maintained macroscopic homogeneity while accelerating rheological and electrokinetic degradation, whereas static storage at 5 °C preserved the rheological state closest to the fresh slurry and caused the smallest zeta-potential shift. For the RT-stored slurries, no systematic increase in maximum particle size was observed. Rheological and electrokinetic results instead indicated degradation at the particle-binder network and particle-liquid interfaces. Coin full-cell tests with 4.4 mAh cm −2 anodes showed that storage effects depended strongly on active-material composition and storage condition. For the silicon-rich formulation, 14 d at RT resulted in approximately 12%–13% greater capacity loss than for cells prepared from the corresponding fresh slurry, whereas storage at 5 °C limited this storage-related increase to ∼3% after the 200-cycle long-term cycling protocol.