12 June 2017 in Physica Status Solidi (a)
Silicon wafer solar cells continue to be the leading photovoltaic technology, and in many places are now providing a substantial portion of electricity generation. Further adoption of this technology will require processing that minimises losses in device performance. A fundamental mechanism for efficiency loss is the recombination of photo‐generated charge carriers at the unavoidable cell surfaces. Dielectric coatings have been shown to largely prevent these losses through a combination of different passivation mechanisms. This review aims to provide an overview of the dielectric passivation coatings developed in the past two decades using a standardised methodology to characterise the metrics of surface recombination across all techniques and materials. The efficacy of a large set of materials and methods has been evaluated using such metrics and a discussion on the current state and prospects for further surface passivation improvements is provided.
1 October 2018 in Solar Energy Materials and Solar Cells
GBGabrielle Bourret-Sicotte
Gabrielle Bourret-Sicotte
+6
1 January 2014 in IEEE Journal of Photovoltaics
Through an advanced hydrogenation process that involves controlling and manipulating the hydrogen charge state, substantial increases in the bulk minority carrier lifetime are observed for standard commercial grade boron-doped Czochralski grown silicon wafers from 250-500 μs to 1.3-1.4 ms and from 8 to 550 μs on p-type Czochralski wafers grown from upgraded metallurgical grade silicon. However, the passivation is reversible, whereby the passivated defects can be reactivated during subsequent processes. With appropriate processing that involves controlling the charge state of hydrogen, the passivation can be retained on finished devices yielding independently confirmed voltages on cells fabricated using standard commercial grade boron-doped Czochralski grown silicon over 680 mV. Hence, it appears that the charge state of hydrogen plays an important role in determining the reactivity of the atomic hydrogen and, therefore, ability to passivate defects.
17 November 2020 in Progress in Photovoltaics: Research and Applications
At present, the commercially dominant and rapidly expanding PV‐device technology is based on the passivated emitter and rear cell (PERC) design developed at UNSW. However, this technology has been found to suffer from a carrier‐induced degradation commonly referred to as ‘light‐ and elevated temperature‐induced degradation’ (LeTID) and can result in up to 16% relative performance losses. LeTID was recently shown to occur in almost every type of silicon wafer, independent of the doping material. Even though the degradation mechanism is known to recover under normal operation conditions, it is a lengthy process that drastically affects the energy yield, stability and, ultimately, the levelized cost of electricity (LCOE) of installed systems. Despite the joint effort of many research groups, the root cause of the degradation is still unknown. Here, we provide an overview of the existing literature and describe key LeTID characteristics and how these have led to the development of various theories of the underlying mechanism. Further, given the continuously appearing and strong evidence of hydrogen involvement in LeTID, many mitigation methods concerning hydrogenation have been suggested. We discuss such reported methods, bearing in mind crucial consumer necessities in terms of sustained cell performance and minimised LCOE.
1 August 2015 in Energy Procedia
Advanced hydrogenation processes targeting the generation of neutrally charged hydrogen (H°) are applied to passivate structural defects in seeded-cast quasi mono-crystalline silicon wafers and boron-oxygen defects in Czochralski silicon. The application of a one minute laser hydrogenation process onto a finished screen printed solar cell fabricated on the dislocation-rich seeded-cast material resulted in efficiency enhancements of 0.6% absolute through improvements in the implied open circuit voltage and internal quantum efficiency in the vicinity of the dislocated regions. A new insight is presented on the formation of boron-oxygen defects with a strong dependence on illumination intensity. An advanced laser hydrogenation process is presented to rapidly form and hydrogenate boron-oxygen defects simultaneously, in an 8 s process applied directly after belt furnace firing, with the hydrogenation of more than 95% of boron-oxygen defects at a peak temperature of approximately 360°C on lifetime test structures. The same 8 s process is also demonstrated on standard screen-printed solar cells applied directly after belt furnace firing to simultaneously form- and hydrogenate the boron-oxygen defects, with no subsequent loss in electrical performance, hence avoiding a 0.7% absolute loss in efficiency due to light-induced degradation
1 January 2013 in Energy Procedia
We report on hydrogen passivation of boron-oxygen defects through manipulation of the hydrogen charge states within the silicon. Standard hydrogenation processes which do not control hydrogen charge states do not appear to passivate a significant quantity of boron-oxygen defects and may result in a reduction in lifetime for wafers with high boron doping concentrations. An improved hydrogenation process through charge state manipulation is observed to lead to substantial improvements in the lifetimes of standard 2Ωcm commercial grade boron-doped Czochralski wafers and experimental compensated 2Ωm Czochralski grown wafers. The passivation of boron-oxygen defects using hydrogen is a fully reversible process, and hence subsequent processes can lead to a net reactivation of boron- oxygen defects if there are insufficient quantities of atomic hydrogen in the correct charge state. Through improved hydrogenation, independently confirmed open circuit voltages in excess of 680mV are demonstrated on solar cells fabricated using standard commercial grade boron-doped Czochralski grown wafers on an industrial production line