15 November 2020 in IEEE Sensors Journal
26 June 2020 in IEEE Transactions on Electron Devices
This article reports the fabrication of zinc-oxide (ZnO) single-nanowire (SNW)-based back-to-back Schottky diodes (BBSDs) using microcantilever-printed AgNP contact pads. ZnO SNWs have been placed on a SiO 2 /Si surface by dropcasting an optimized dispersion of ZnO nanowires (NWs) in deionized (DI) water. The microcantilever-printing process has been used to overlap the surface of the ZnO NW with the AgNP pads. The electrical response of the printed diodes has been verified with an analytical model based on the thermionic emission theory. Printed-Schottky diodes have been fabricated with varying channel lengths of ZnO SNW, and among them, the typical ideality factor of ~2.4, the lowest Schottky barrier height of 0.21 eV for the positive voltage sweep and 0.17 eV for the negative voltage sweep, the ${I}_{ \mathrm{\scriptscriptstyle ON}}/{I}_{ \mathrm{\scriptscriptstyle OFF}}$ ratio in the order of $\sim 10^{{3}}$ – $10^{{4}}$ , the lowest series resistance of 30 $\text{k}\Omega $ , and the fastest turn-on voltage of 50 mV have been obtained. The reported fabrication process is simple, reproducible, and repeatable and of low cost in nature.
7 June 2021 in IEEE Electron Device Letters
Inorganic semiconductors have the potential features to enhance the stability and performance of printed electronic devices. In this work, we present a microcantilever (μC) printed device by using zinc oxide (ZnO) and silver nanoparticles (AgNP) ink. Two types of devices have been fabricated on silicon wafers using two methods: (i) the ZnO ink is printed between two μC printed AgNP electrodes separated within a sub-5 μm gap (ii) the ZnO ink have been drop-casted between two μC printed AgNP electrodes. Therefore the first type of devices is a fully printed structure. The measurements of both devices show distinct electrical aspects corresponding to the different additive fabrication approach. Furthermore, the fully printed Schottky diode exhibits a remarkable high on/off current ratio of 1.85 × 105 at room temperature with a barrier height of 0.49 eV and series resistance of 594 kΩ.
12 April 2022 in IEEE Sensors Journal
This work describes the fabrication of a Carbon monoxide (CO) sensor based on a Zinc oxide (ZnO) Schottky diode that can detect CO at low concentrations as low as one part per million (ppm) at room temperature. Different additive microfabrication techniques are used to fabricate the devices. A precisely controlled fabrication is enabled by employing a microcantilever ( $\mu \text{C}$ ) printing system. The fully printed sensor has a high sensitivity of 23.7% towards CO at room temperature. The height of the Schottky barrier significantly influences the response of the device. Furthermore, all sensors specificity was analyzed for some of the gases, and volatile organic compounds (VOCs) found in breath. The fully printed device exhibited a negative temperature coefficient of resistivity for temperatures ranging from 50 to 300 Kelvin. This work aims to develop a proof-of-concept for enhancing room temperature sensing by developing a Schottky sensor.
6 April 2021 in IEEE Transactions on Nanotechnology
This work reports the fabrication of ZnO single-nanowire (SNW) Schottky diode based-sensors with micro-cantilever printed AgNP contact pads, for room temperature (RT) detection of air pollutants such as CO 2 and CO. ZnO SNWs with length in range of ~ 1-5 μm and diameter in the range of ~ 90-250 nm have been placed on a silicon substrate by drop-casting an optimized dispersion of ZnO nanowires in de-ionised (DI) water. ZnO nanowire dispersion is further optimized by adding sodium dodecyl sulfate (SDS) and acetic acid to form longer nanowires which ease the reproducibility and scaling of the fabrication process. The sensors demonstrate a wide gas-sensing range of 500 ppb to 500 ppm and 10 ppb to 9 ppm for CO 2 and CO respectively. A higher sensitivity of 0.34%/ppm and 0.28%/ppm is obtained for CO 2 and CO respectively. It is found that SDS treatment makes sensors more selective towards CO 2 and CO. The fabricated sensors show a low response time mostly in a range of ~ 5-10 s and recovery time in a range of ~ 2-10 minutes. These sensors are stable within a relative humidity range of (15-75)%.
2 February 2021 in IEEE Sensors Journal
The fabrication and testing of hierarchical architecture based Zinc Ferrite-Zinc oxide (ZnFe 2 O 4 -ZnO) magnetic semiconductor (MS) sensor, for the detection of Hydrogen (H 2 ) down to 50 parts per million (ppm) at room temperature, are reported in this study. The synthesis of ZnFe 2 O 4 -ZnO heterostructure has been carried out using a simple hydrothermal route. The MS sensor shows good sensitivity, quick response, and remarkably good recovery to H 2 at room temperature. A rise in the magnetic movement is verified in ZnFe 2 O 4 -ZnO heterostructure with the interaction of reducing H 2 gas. The sensor exhibits a detection limit of 8.9 ppm with the highest sensitivity of 20% for the detection of 900 ppm of H 2 , with a response time of 35-55 s. The sensitivity of the MS sensor towards some of the breath volatile organic compounds (VOCs) and cross-sensitivity of H 2 and carbon dioxide (CO 2 ) are analysed. The work is aimed to provide a straightforward approach for the H 2 breath test using magnetic particles that have the potential to become a portable device for diagnostics.