Gaoyuan Hou

Gaoyuan Hou

Auto-generated profile, based on publicly available information

Gaoyuan Hou

Department of Biomaterials Science, Graduate School of Agricultural and Life Sciences, The University of Tokyo, Tokyo, Japan

Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
16 June 2020 in ACS Applied Materials & Interfaces
Verified
Journal Article
Closed access
GHGaoyuan Hou
Gaoyuan Hou
YLYu Liu
Yu Liu
DZDejian Zhang
Dejian Zhang
GLGuanhui Li
Guanhui Li
HXHong Xie
Hong Xie
ZFZhiqiang Fang
Zhiqiang Fang

12 July 2022 in Cellulose
Verified
Journal Article
Closed access
PDF file
GHGaoyuan Hou
Gaoyuan Hou
SZSishun Zhao
Sishun Zhao
LPLiyuan Peng
Liyuan Peng
ZFZhiqiang Fang
Zhiqiang Fang
AIAkira Isogai
Akira Isogai


6 July 2024 in Carbohydrate Polymers
Verified
Journal Article
Open access
KCKorawit Chitbanyong
Korawit Chitbanyong
GHGaoyuan Hou
Gaoyuan Hou
MTMiyuki Takeuchi
Miyuki Takeuchi
ISIzumi Shibata
Izumi Shibata
AIAkira Isogai
Akira Isogai
Three commercial regenerated cellulose samples were subjected to TEMPO-catalyzed oxidation using solid NaOCl·5H2O as the primary oxidant for structural analyses of the oxidized products (TEMPO = 2,2,6,6-tetramethylpiperidine-1-oxyl). The regenerated cellulose/water slurries became transparent solutions after oxidation for 60 min. The yields of the oxidized products were almost 100 % when they were isolated as precipitates in ethanol/water mixtures. The solution-state NMR spectra revealed that the oxidized products were almost pure water-soluble β-(1 → 4)-polyglucuronic acids; the reaction conditions described herein ensured the complete oxidation of the C6-OH groups in the regenerated cellulose samples to C6-carboxy groups. However, the solid-state 13C NMR spectra of the oxidized products indicated that C2/C3-ketones (<20 % of the total units) were formed during side reactions, which is characteristic for oxidized products prepared from regenerated cellulose with the C2/C3-glycol structure. These ketones were likely to form intermolecular hemiacetal linkages in the oxidized products. During conductivity titration of the oxidized products, it is necessary to control the sample masses to accurately determine the carboxy contents. The mass-average degree of polymerization decreased from 330 to 890 for the original regenerated cellulose samples to 65-79 for the oxidized products; substantial depolymerization is inevitable during TEMPO-catalyzed oxidation of the regenerated cellulose samples.

12 January 2024 in Carbohydrate Polymers
Verified
Journal Article
Closed access
KCKorawit Chitbanyong
Korawit Chitbanyong
GHGaoyuan Hou
Gaoyuan Hou
ISIzumi Shibata
Izumi Shibata
MTMiyuki Takeuchi
Miyuki Takeuchi
SKSatoshi Kimura
Satoshi Kimura
AIAkira Isogai
Akira Isogai

15 July 2025 in Carbohydrate Polymers
Verified
Journal Article
Open access
GHGaoyuan Hou
Gaoyuan Hou
KCKorawit Chitbanyong
Korawit Chitbanyong
ISIzumi Shibata
Izumi Shibata
AIAkira Isogai
Akira Isogai
Phosphorylated (P-) and TEMPO-oxidized (TO-) wood cellulose fibers (pulps), and P- and TO-cellulose nanofibrils (CNFs) were prepared. To extract pure cellulose molecules, all samples were dispersed in water and freeze-dried, and the P-/TO-pulp and P-/TO-CNF samples were stirred in 8 % (w/w) lithium chloride/N,N-dimethylacetamide (LiCl/DMAc). The quantities of the extracted LiCl/DMAc-soluble fractions and molar-masses of the constituents were determined using size-exclusion chromatography. The structures of the LiCl/DMAc-insoluble fractions were analyzed using X-ray diffraction (XRD) and solid-state 13C-nuclear magnetic resonance (NMR). The mass ratios of the LiCl/DMAc-extracted fractions obtained from the P-/TO-pulp and P-/TO-CNF samples were in the low range of 2-9 %, consisted with the hypothesis that structurally, all the cellulose molecules in each cellulose microfibril of the P-/TO-pulp and P-/TO-CNF samples possess some phosphate ester groups or C6-carboxy groups. These cellulose molecules containing phosphate ester groups or C6-carboxy groups were insoluble in LiCl/DMAc. XRD and NMR analyses of the LiCl/DMAc-insoluble fractions of the TO-pulp samples showed that the cellulose I crystal structures inside the cellulose microfibrils were transformed into disordered structures by pretreatment with EDA. In contrast, the cellulose I crystal structure of the P-pulp was stable in EDA and was retained after post-treatment.