27 June 2022 in Applied Physics Letters
In situ ion-beam-induced luminescence measurements reveal a strong enhancement of the Cr3+ emission yield in electrically conductive chromium doped β-Ga2O3 single crystals upon proton irradiation. The observed effect can be explained based on the Fermi-level pinning caused by radiation defects. This pinning of the Fermi level activates deep carrier traps that can act as sensitizers of the Cr3+ emission. In agreement with this model, in semi-insulating samples, where the Fermi level lies deep in the bandgap, the Cr3+ emission is present already in as-grown samples, and no enhancement of its intensity is observed upon proton irradiation. The boost of the Cr3+ emission yield by irradiation, observed in conductive samples, is reversed by thermal annealing in argon at temperatures above 550 °C for 30 s. The results reveal a high potential of Cr-doped β-Ga2O3 for in situ and ex situ optical radiation detection and dosimetry.
18 March 2020 in Journal of Applied Physics
Tb Sc Al O (TSAG) is a paramagnetic insulator which, in spite of its congruent nature and excellent magneto-optical properties as Faraday rotators for optical isolators (OIs), cannot be industrially produced. The reason is that its lattice structure is so stressed that single crystals easily crack upon cooling after growth or during the cutting process. By the incorporation of a small amount of Lu, it has been demonstrated that the stress in the structure can be effectively released, and, therefore, the crystal cracking can be avoided. This has enabled the substitution of standard Tb Ga O (TGG), achieving better high-power performance and compacter OIs. In this study, the charge state and the lattice site location of Lu as well as Y dopants in TSAG are investigated by X-ray Absorption Near Edge Structure and Extended X-ray Absorption Fine Structure Analysis. Measurements on single crystal and powdered samples indicate that both dopants are incorporated in the 3+ charge state and substitute predominantly in the dodecahedral Tb-site ( 87.5%), while a minor fraction is found in the octahedral Sc-site.
1 January 2021 in Journal of Synchrotron Radiation
15 January 2004 in Journal of Magnetism and Magnetic Materials
1 October 2022 in Journal of Applied Crystallography
Micro-Laue diffraction has been used to record cross-section profiles on a quasi-lattice-matched HgCdTe/CdZnTe heterostructure as a function of the stress induced by a flexion machine. The heterostructure may be decomposed into four different regions according to depth. Sufficiently far from the interface, the CdZnTe substrate is undisturbed by the HgCdTe layer, while the region situated 10 µm beneath the interface presents an in-plane lattice parameter adjustment to the +0.02% mismatched layer. The layer has a 2 µm critical thickness and, beyond, misfit dislocations induce a large peak broadening whose main direction changes with depth. The same occurs over the whole heterostructure once flexion-induced plastification has started. Consequently, the usual full width at half-maximum or integral breadth is no longer relevant, and only a newly defined and rotationally invariant 2D integral breadth correctly measures the plastification-induced peak broadening. Taking into account only the critical thickness region, a 15.1 ± 0.7 MPa tensile HgCdTe elastic limit was measured, slightly overestimated because of the initial compressive layer stress. It was observed that the plastic onset of the substrate perfectly matches the elastic limit of the layer, despite the fact that the substrate elastic limit is expected to be four times higher: a striking demonstration of the propagation of threading dislocations. The `plastification easiness' is found to be 2.4 times smaller deep inside the substrate than in the layer critical thickness region, while in the substrate lattice adjustment region, the plastification easiness goes from the substrate to the layer value with a 22–25 MPa transition interval. This novel method using the 2D integral breadth allows for easy critical thickness measurement as well as precise plastic onset determination and plastification easiness assessment. It is a quite general method, since it may be applied to the vast class of epitaxial layers for which the critical thickness is larger than the micro-Laue beam size (currently 250 nm).