1 November 2021 in Journal of Molecular Liquids
6 December 2022 in Chimica Techno Acta
RARayana K. Abdurakhimova
Silicon and silicon-based materials are increasingly used in microelectronics, metallurgy and power generation. To date the active study aimed at the development of silicon materials to be used in devices for solar energy conversion, accumulation and storage is underway. In addition, silicon is a promising anode material for lithium-ion fuel cells. In the present paper a possibility of silicon electroreduction from the NaI–KI–K2SiF6 melt in the argon atmosphere is studied. With this aim in view the electrolysis of the NaI–KI–K2SiF6 melt with glassy carbon cathode was performed under galvanostatic and potentiostatic regimes at the temperatures ranging from 650 to 750 °С. The morphology, phase and elemental analyses of the obtained silicon deposits were performed after their separation from the electrolytes by the ICP, SEM-EDX, XRD and Raman spectroscopy methods. Fiber and thread-like silicon samples of 60 to 320 nm in dimeter with admixtures concentrations (mainly oxygen) from 1.2 to 4.6 wt.% were experimentally synthesized. The obtained samples were tested as possible Si/C composite anodes for lithium-ion power sources. The discharge capacity of such power sources after 30 cycles of lithiation-delithiation ranged from 440 to 565 mAh·g–1 and the coloumbic efficiency ranged from 89 to 91%.
1 January 2021 in Journal of the Serbian Chemical Society
The regularities of silicon and aluminum co-deposition on glassy carbon from KF?KCl (2:1)?75 mol % KI?0.15 mol % K2SiF6?(up to 0.15 mol %) AlF3 melts at 998 K were studied by cyclic voltammetry, chronoamperometry, scanning electron microscopy, atomic force microscopy and Raman spectroscopy. The cyclic voltammograms demonstrated the presence of only one cathodic peak (or nucleation loop at a low reverse potential) and the corresponding anodic peak. The cathodic peak shifted in the cathodic direction with decreasing concentration of aluminum ions in the melt or with increasing scan rate. The Scharifker?Hills model was used to analyze potentiostatic current density transients and estimate the values of the apparent diffusion coefficient and the number density of nuclei. The morphology and elemental analysis of the samples obtained during potentiostatic and galvanostatic deposition for 30?60 s were studied. Continuous thin silicon films doped with aluminum were obtained under galvanostatic conditions.
13 July 2018 in Journal of the Electrochemical Society
The rhenium electrodeposition from the KF-KBF4-B2O3-KReO4 melts at 773 K was studied by the cyclic voltammetry. Two waves were found on the E(i) dependences in the cathode region corresponding to the reduction of Re (VII) to metallic Re: Re7++3e→Re4+, and Re4++4e→Re0. The galvanostatic electrolysis in the KF-KBF4-B2O3-KReO4 melt in an atmosphere of an ambient air was performed. It was revealed that the use of the KF-KBF4-B2O3-KReO4 electrolyte (with 5.4 wt% Re) provides the Re electrowinning on the Re substrate during 20 h at 773 K without a decrease in the rhenium ions concentration. The electrolytic deposits were analyzed by the XRD, SEM-EDS and ICP-AES spectroscopy. It was demonstrated that the electrolytic deposits were the metallic Re with a purity of 99.98 wt%. The operating conditions for producing the Re deposit with a current efficiency of 98% were determined.
1 November 2018 in Journal of Physics: Conference Series
The electrochemical behavior of Si4+ deposited onto the Cu substrate, in comparison with one onto C substrate, in the KF-KCl-KI-K2SiF6 melt was investigated by the cyclic voltammetry at 993 K. It was found, that the electro reduction of silicon on the Cu substrate proceeds with formation of the Cu-Si alloy (silicon bronze). The electrolysis conditions were determined and the silicon bronze coatings were synthesized by electrolysis in the KF-KCl-KI-K2SiF6 melt. The surface of deposits was examined by the electron microsccopy with EDS analysis. The deposits contained only copper and silicon. The microhardness of the coatings achieved 1618 HV. The microhardness of the obtained films was tested in air during one month: it decreased from 1618 to 380 HV.
1 February 2022 in Russian Metallurgy (Metally)
The surface tension of the KF–KCl–KI salt melts with an unchanged KF/KCl molar ratio is measured as a function of the KI content using a platinum cylinder detachment method. The measurements are performed in an inert atmosphere using structural materials stable against the melts under study. The surface tension of the (66KF–34KCl)–KI (mol %) melts with KI/(KCl + KF) molar ratios of 0–100% is measured in a temperature range of 863–1083 K. KI added to the KF–KCl melt is found to decrease the surface tension. The temperature dependences of the surface tension of the melts are described by linear functions. An increase in the KI concentration is shown to decrease the coefficient of the temperature dependence of the surface tension.