1 December 2017 in Solar Energy Materials and Solar Cells
22 September 2016 in IEEE Journal of Photovoltaics
Light-induced or, more broadly, carrier-induced degradation (CID) in high-performance multicrystalline silicon (TIP mc-Si) solar cells remains a serious issue for many manufacturers, and the root cause of the degradation is still unknown. In this paper, the impact of firing temperature on the stability of lifetime test structures is investigated, and it is found that substantial CID can be triggered if peak temperatures exceed approximately 700 °C. We then investigate two pathways to stabilize the performance of industrially produced TIP mc-Si passivated emitter rear contact cells which have been fired at CID-activating temperatures (~740 °C-800 °C) currently required for silver contact formation. The first is a fast-firing approach, whereby it is demonstrated that an additional firing step at a reduced temperature after cell metallization can suppress the extent of V oc degradation by up to 80%. The second approach is the accelerated degradation and subsequent recovery of carrier lifetime through the use of high-intensity illumination during annealing at elevated temperatures. A 30 s process is found to suppress the maximum extent of degradation in V oc by up to 60% and up to 80% for longer processes. Ultimately, the results suggest that a combined approach of fast-firing and a high-intensity-illuminated anneal could achieve the best results in terms of V oc , stability.
11 January 2018 in IEEE Journal of Photovoltaics
Carrier-induced degradation (CID) of multicrystalline silicon (mc-Si) solar cells has been receiving significant attention; however, despite this increasing interest, the defect (or defects) responsible for this degradation has not been determined yet. Previous studies have shown that the surface passivation layer and the firing temperature have a significant impact on the rate and extent of this degradation. In this paper, we further study this impact through an investigation of the CID behavior of the mc-Si wafers passivated with six different silicon nitride layers, each fired at four different peak temperatures. At low firing temperatures, no significant difference in the CID was identified between the samples with different passivation layers; however, a large range of degradation extents was observed at higher firing temperatures. Using Fourier transform infrared spectroscopy, a correlation was found between the degradation extent and the amount of hydrogen released from the dielectric during firing. We verified that no degradation of the surface passivation quality occurred, indicating that the degradation is primarily associated with a bulk defect.
6 February 2017 in Solar RRL
1 September 2018 in Solar Energy Materials and Solar Cells
20 January 2016 in Physica Status Solidi (RRL) – Rapid Research Letters