The magnon propagation length (MPL) is one of the crucial factors to govern spin transport in a magnetic material. Here, we determine MPL (ξ) in compensated ferrimagnetic Gd3Fe5O12 (GdIG) thin films at room temperature by investigating longitudinal spin Seebeck effect (LSSE) in Gd3Ga5O12(GGG)/GdIG(t)/Pt(5nm) heterostructures with different thicknesses (t) of the GdIG film. All films possess in-plane (IP) magnetic easy axis, and the compensation temperature shifts down to lower temperature with decreasing GdIG thickness. At room temperature, the LSSE signal is rather constant with thickness between t = 221 and 89 nm, but drops significantly below t = 50 nm. By fitting the thickness dependence of the LSSE voltage to a modified atomistic spin model considering the influence of saturation magnetization, we obtain ξ = 45 ± 8 nm for GdIG thin films at room temperature. The MPL of GdIG is much shorter than that of Y3Fe5O12 films (ξ~90 -140 nm), but higher than that of Fe3O4 films (ξ~20 nm). The obtained value of ξ explains the drop in the LSSE voltage in GdIG films when the film thickness is reduced below 50 nm, knowledge of which is also essential to the design of spincaloritronic devices based on GdIG films.
Rare-earth iron garnets (REIGs) are the benchmark systems for magnonics, including the longitudinal spin Seebeck effect (LSSE). While most research has focused on single-crystalline REIGs on complimentary garnet substrates, moving to more, cost-effective complementary metal-oxide semiconductor (CMOS)-compatible substrates is important to integrate REIG thin films with existing technology. In this regard, we grow a 130 nm-thick polycrystalline gadolinium iron garnet (GdIG) film on the Si/SiO2 substrate and investigate the temperature-dependent LSSE. Interestingly, the polycrystalline GdIG film exhibits perpendicular magnetic anisotropy (PMA) at room temperature which is induced by tensile in-plane (IP)-strain originating from the thermal-expansion mismatch between the GdIG film and the substrate during rapid thermal annealing. Further, a spin-reorientation transition from the out-of-plane IP direction below TS = 180 K is observed. Additionally, the film reveals a magnetic compensation temperature, TComp, of ≈240 K. The LSSE voltage not only demonstrates a sign-inversion around TComp, but also shows noticeable changes around TS. As compared to a single-crystalline GdIG film, the lower LSSE voltage for the polycrystalline GdIG is attributed to the higher effective magnetic anisotropy and enhanced magnon scattering at the grain boundaries. Our study not only paves the way for the cost-effective growth of CMOS-compatible REIG-based systems with PMA for magnonic memory and information processing applications, but also highlights the fact that the spincaloritronic and spin-insulatronic properties of the polycrystalline REIGs follow those of their single-crystalline counterparts with reduced spin-to-charge conversion efficiency through LSSE which can be tuned further by controlling the average gran size and interface engineering.