Fabiano Perez

Fabiano Perez

Auto-generated profile, based on publicly available information

Fabiano Perez

Faculdade São Leopoldo Mandic

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
6 February 2022 in Research, Society and Development
Verified
Journal Article
Open access
PDF file
SVSelem Alvarenga Vilela
Selem Alvarenga Vilela
AFAline Batista Gonçalves Franco
Aline Batista Gonçalves Franco
GCGeraldo Alberto Pinheiro de Carvalho
Geraldo Alberto Pinheiro de Carvalho
SDSérgio Candido Dias
Sérgio Candido Dias
SJSilvio Mecca Junior
Silvio Mecca Junior
CMCaio Marques Martins
Caio Marques Martins
The aim of this study is to analyze the compressive strength of occlusal splints manufactured with three different liquid resins in a 3D printer and in three angles of orientation. The resins used here are (n=12): Resilab Clear (Wilcos do Brasil, Petrópolis, RJ, Brazil), Prizma Smart Print Bio (Makertech Labs, Tatuí, SP, Brazil), and Cosmos Splint (Yller Biomateriais, Pelotas, RS, Brazil); each resin group are divided into three subgroups according to orientation of manufacture: 0, 45 and 90 degrees. A dental manikin was scanned and the file was used to manufacture a steel hemiarch model. This model was used to design the occlusal splints and as a basis for the tests. The splints were designed with flat occlusal surface and minimum thickness of 2 mm. The compressive test was performed with constant force of 200N, velocity of 0.5 mm/min, along the entire occlusal surface until fracture. Results show no difference between the resins, regardless of orientation of manufacture. The orientation showed no intragroup effect for resins Prizma Smart Print Bio and Resilab Clear; the resin Cosmos showed larger compressive strength for the samples manufactured at 45 degrees than at 0 degree. The 90-degree samples were intermediary and showed no difference from other angles. This study shows that the three resins had similar behavior in terms of compressive strength, except for the intragroup effect of orientation of Cosmos Splint resin, where plates manufactured at 0 degree performed worse than those at 45 degrees.

17 April 2022 in Research, Society and Development
Verified
Journal Article
Open access
PDF file
TFTácio Gonçalves Nogueira Fonseca
Tácio Gonçalves Nogueira Fonseca
GCGeraldo Alberto Pinheiro de Carvalho
Geraldo Alberto Pinheiro de Carvalho
CMCaio Marques Martins
Caio Marques Martins
SJSilvio Mecca Junior
Silvio Mecca Junior
FPFabiano Perez
Fabiano Perez
AFAline Batista Gonçalves Franco
Aline Batista Gonçalves Franco
The present study assesses the shear strength of Polyether Ether Ketone (PEEK) and Zantex to thermopolymerizable acrylic resin (TAR) with different surface treatments. To this end, 100 test specimens were produced and divided into two groups: G1(PEEK + TAR) and G2 (Zantex + TAR). Each group was subdivided into the subgroups A, B, C, D and E (n=10) according to surface pre-treatment: A: TAR + PEEK/Zantex without surface treatment (control); B: TAR + PEEK/Zantex treated with Palabond; C: TAR + PEEK/Zantex blasted with aluminum oxide (Al2O3) of 125 µm; D: TAR + PEEK /Zantex treated with Al2O3 of 125 µm + Palabond; and E: TAR + PEEK/Zantex prepared with groove-shaped retentions. The structures were tested in a Universal testing machine EMIC DL2000. Two-way variance analysis showed significant difference between materials and surface treatments (p < 0.001). Multiple comparisons were done with Tukey’s test and failure modes were analyzed with the G test. Statistical analysis showed that Zantex outperformed PEEK for most treatments and showed similar performance in the subgroups treated with Al2O3. Within the PEEK group, the use of grooves and Palabond combined with blasting showed the best results; in the Zantex group, the best results were obtained with Palabond and Palabond combined with blasting. Regarding failure modes, PEEK showed only adhesive failures and Zantex’s failures were dependent on treatment. Therefore, the surface treatment method applied to the polymers studied here contribute to the material’s adhesion to acrylic resin.

13 May 2022 in Research, Society and Development
Verified
Journal Article
Open access
PDF file
RNRoberto Burguer Neto
Roberto Burguer Neto
AFAmanda Gonçalves Franco
Amanda Gonçalves Franco
GCGeraldo Alberto Pinheiro de Carvalho
Geraldo Alberto Pinheiro de Carvalho
CMCaio Marques Martins
Caio Marques Martins
SJSilvio Mecca Junior
Silvio Mecca Junior
AFAline Batista Gonçalves Franco
Aline Batista Gonçalves Franco
The aim of this study is to test and compare the flexural strength of milled polymer bars, with and without glass fiber reinforcement. The number of samples in the study was defined through a pilot study on a universal testing machine (EMIC) (n = 5). The brands analyzed in this study were Arch Free Metal, Zantex, Bioplas and PEEK. All samples were submitted to thermal aging before the three-point flexural test. Fracture patterns were analyzed using a Scanning Electron Microscope. Results show that the Arch Free Metal bar presented the largest flexural strength, followed by Zantex and PEEK bars, that lacked statistical difference, and Bioplas bars. Regarding fracture patterns, Arch Free Metal and Zantex bars were partially fractured and showed partial glass fiber rupture; PEEK bars were not fractured and showed plastic behavior; and Bioplas bars were fractured. It is possible to conclude that the reinforced polymer bar Arch Free Metal has a better performance in terms of flexural strength than the other tested materials.

9 March 2022 in Research, Society and Development
Verified
Journal Article
Open access
PDF file
FFFrancisco Fernando Massola Filho
Francisco Fernando Massola Filho
AFAmanda Gonçalves Franco
Amanda Gonçalves Franco
GCGeraldo Alberto Pinheiro de Carvalho
Geraldo Alberto Pinheiro de Carvalho
SDSérgio Candido Dias
Sérgio Candido Dias
ERElimario Venturin Ramos
Elimario Venturin Ramos
AFAline Batista Gonçalves Franco
Aline Batista Gonçalves Franco
The aim of this study is to assess how shear strength of Ultra Translucent Multi Layered Zirconia Katana (UTML) is affected by the conditioning with 10% hydrofluoric acid combined with the current surface treatment protocol: air, primer containing 10-MDP, and cement. Samples of UTML Zirconia Katana were machined to measure 5x5x10 units of measurement, attached, and divided into two groups. In the control group, samples were treated with 27 um aluminum oxide blasting at 4 bars, application of Zr primer containing 10-MDP and, finally, cement Panávia V5. In the experimental group, samples were also treated with 10% hydrofluoric acid following blasting and prior to the primer application. The test specimens were submitted to shear mechanical strength test on a universal testing machine EMIC DL2000 (EMIC, São Paulo, Brazil), surface analysis with Scanning Electron Microscope (SEM) (Sputter Coaster Emitech, K450) and surface roughness. Results showed that the bond strength of specimens conditioned with acid was 41% higher (p = 0.031). Student’s t test showed that the samples conditioned with acid were rougher than those without conditioning (p = 0.045). Microscopic analysis showed surface alterations on samples conditioned with acid. It is possible to conclude that the group conditioned with hydrofluoric acid showed better adhesive behavior.

6 February 2022 in Research, Society and Development
Verified
Journal Article
Open access
PDF file
MMMariana Cristina Teixeira Martins
Mariana Cristina Teixeira Martins
AFAmanda Gonçalves Franco
Amanda Gonçalves Franco
GCGeraldo Alberto Pinheiro de Carvalho
Geraldo Alberto Pinheiro de Carvalho
SDSérgio Candido Dias
Sérgio Candido Dias
CMCaio Marques Martins
Caio Marques Martins
AFAline Batista Gonçalves Franco
Aline Batista Gonçalves Franco
The aim of this study is to assess the bond strength of three resinous cements to Zirconia Katana™ UTML (Kuraray Noritake Dental Inc, Miyoshi, Aichi, Japan). Thirty-six blocks of Zirconia were milled and included in polyvynil chloride (PVC) pipes with self-polymerizable acrylic resin. Each sample was polished in a polishing machine, blasted with aluminum particles, cleaned with ultrasound, and dried with compressed air. The cementation was done according to the protocol recommended by the manufacturer. The samples were divided in 3 groups (n=12) according to the resinous cement used: Group R - RelyX™ U200 Automix (3M ESPE, Sumaré, São Paulo, Brazil); Group M - Multilink® N (Ivoclar Vivadent, Schaan, Liechtenstein); and Group P - Panavia™ V5 Paste (Kuraray Noritake Dental Inc, Cotia, São Paulo, Brazil). The shear stress test was performed in EMIC DL2000 (EMIC, São Paulo, SP, Brazil), and failure type was analyzed. Average bond strengths were 5.4 kgf, 5.8 kgf, and 6.68 kgf for groups R1, M1 and P1, respectively. Variance analysis showed no significant difference between groups. None of the groups showed cohesive failure; there was no significant difference in the frequency of mixed and adhesive failure between groups. All three cements showed similar performance in the tests.