Pavel E. Yudin

Pavel E. Yudin

Auto-generated profile, based on publicly available information

Pavel E. Yudin

Samara State Technical University; Scientific and Production Center “Samara

Research Focus & Metrics

Academic Career Length

3Years (2024-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
6 March 2025 in International Review of Applied Sciences and Engineering
Verified
Journal Article
Open access
PDF file
DBDenis V. Berkov
Denis V. Berkov
IKIvan I. Kostyuk
Ivan I. Kostyuk
PYPavel E. Yudin
Pavel E. Yudin
AVAlexander G. Verevkin
Alexander G. Verevkin
The inorganic scaling in wells is a common problem faced by mining companies. At present, the use of protective coatings for tubing as a measure to prevent or reduce the formation of inorganic scale deposits on pipe walls has not been fully studied. To use protective coatings as a measure to counteract the deposition of inorganic salts, it is necessary to develop a method that allows assessing the ability of coatings, as well as polymer and metal materials, to prevent the formation of inorganic scale deposits on the inner surface of pipes.The article proposes a method for assessing the ability of protective coatings to resist the inorganic scaling on the inner surface of tubing. The proposed assessment method allows to make an informed decision on the advisability of using internal protective coatings of tubing to prevent (or reduce) the formation of inorganic scale deposits. The authors consider design features of a test bench for assessing the resistance of coatings to inorganic scale deposits, which allows to simulate the conditions for the formation of scale deposits that are as close as possible to the real conditions of oil production facilities. The article presents the results of bench tests of nine coating samples, two polymer samples and one sample made of St 40G2 steel. To assess the effectiveness of using tubing with an internal anti-corrosion coating as a measure to combat scale deposits, additional research is required to assess the possibility of complex use of coatings in conjunction with other methods of preventing processes of inorganic scaling. Thus, the authors developed the Bench for assessing the resistance of protective coatings of tubing to inorganic scale deposits. A dynamic testing technique is proposed to evaluate the resistance of protective coatings to inorganic scale deposits. Based on the presented results, conclusions were drawn about the possibility of using protective coatings on tubing as a measure to prevent the formation of inorganic scale deposits on the inner surface of the tubing.

20 May 2024 in Safety of Technogenic and Natural Systems
Verified
Journal Article
Open access
PDF file
ESE. S. Surgaeva
E. S. Surgaeva
PYP. Е. Yudin
P. Е. Yudin
AAAleksandr Petrovich Amosov
Aleksandr Petrovich Amosov
Introduction. Failure of equipment, specifically pipes in the oilfield complex, due to the development of corrosion processes leads to numerous losses, destruction of expensive components, disruption of technological processes and, as a result, environmental damage. The use of anticorrosive coatings as an internal protection of oilfield pipes offers many advantages and can significantly reduce the rate of corrosion, but does not provide a complete solution to this problem. Destruction of internal anticorrosive polymer coatings (IACPC) occurs for numerous reasons. The causes and mechanisms of destruction are insufficiently investigated. Therefore, the aim of this work was to analyze the destruction of internal anticorrosive polymer coatings using practical examples, which made it possible to form and identify the main causes of damage and degradation of coatings during operation.Materials and Methods. A complex of laboratory studies was carried out to study the damage to internal polymer anticorrosive coatings during operation and to establish the main causes of destruction. The initial phase of the investigation involved a detailed examination of the materials related to the accident circumstances, including the operating conditions of the coated pipeline (composition of the operating medium, temperature, pressure, and presence of mechanical impurities), operation time, and type of polymeric material used. The second phase involved laboratory testing of the coating, which included the determination of layer thickness, dielectric continuity, adhesive strength (by the normal separation method), investigation of thermokinetic properties by means of differential scanning callometry (DSC), study of the coating structure using scanning electron microscopy.Results. Practical examples of the destruction of internal anticorrosive coatings of oilfield pipes were analyzed. For each case, characteristic signs of degradation of the anti-corrosive coating were identified. Changes in the microstructure of the coatings, as well as the formation of corrosion products, were observed depending on the type of destruction. The focus was on studying the degree of polymerization of the coating, both using the traditional method of determining the ΔTg parameter using DSC, and based on indirect signs detected during microscopic studies.Discussion and Conclusion. The practical cases of damage to the internal anticorrosion coating of pipes of the oil and gas complex considered in the article allowed us to divide the causes of destruction into three groups: operational, technological and defects during transportation, storage and construction and installation works. Based on these findings, we have formulated recommendations for manufacturers to ensure maximum performance from their coatings. It is noted that the compliance with the presented recommendations makes it possible to obtain internal anticorrosive polymer coatings with a minimum guaranteed lifespan of 15 years, as demonstrated by the successful operations of pipelines in Western Siberia, such as those operated by Surgutneftegaz PJSC and LUKOIL – Western Siberia LLC.

23 May 2026 in Image Journal of Advanced Materials and Technologies
Verified
Journal Article
Closed access
PYP. E. Yudin
P. E. Yudin
MBM. V. Bogatov
M. V. Bogatov
ALAleksandr Lozhkomoev
Aleksandr Lozhkomoev
The paper examines the impact of hydrogen sulfide (H 2 S) on the adhesion strength of internal polymer coatings designed to safeguard oil pipelines against corrosion. The analysis focuses on the mechanisms of coating destruction in aggressive environments, including the chemical reaction of H 2 S with inorganic fillers such as iron oxide (Fe 2 O 3 ), which leads to the formation of sulfides and a sharp decrease in adhesion. Experiments were conducted under autoclave conditions with varying H 2 S concentrations, temperatures, and holding times. The results showed that even minimal H 2 S concentrations significantly deteriorate the adhesive properties of coatings. A model of adhesion reduction is proposed that allows to predict the service life of coatings under specific operating conditions. Particular attention is given to comparing various types of coatings, including duplex, liquid, and powder systems, as well as the role of phenolic primers in their stability. The processes of diffusion and chemical interaction with the coating components were found to play a key role in durability. These findings are crucial for developing more effective anti-corrosion solutions in the oil and gas industry.

25 December 2024 in Bulletin of the Siberian State Industrial University
Verified
Journal Article
Open access
PDF file
MKMaria Kudryashova
Maria Kudryashova
SPSergei S. Petrov
Sergei S. Petrov
PYPavel E. Yudin
Pavel E. Yudin
AEAleksandr Yu. Ezhov
Aleksandr Yu. Ezhov
OBOl'Ga S. Bondareva
Ol'Ga S. Bondareva
АМАлексей Александрович Мельников
Алексей Александрович Мельников
INFLUENCE OF HYDROGEN ABSORPTION ON DESTRUCTION AND MECHANICAL CHARACTERISTICS OF TITANIUM ALLOY | Kudryashova | Bulletin of the Siberian State Industrial University ИССЛЕДОВАНИЕ ВЛИЯНИЯ НАВОДОРОЖИВАНИЯ НА РАЗРУШЕНИЕ И МЕХАНИЧЕСКИЕ ХАРАКТЕРИСТИКИ ТИТАНОВОГО СПЛАВА | Кудряшова, | Вестник Сибирского государственного индустриального университета

30 September 2026 in Frontier materials & technologies
Verified
Journal Article
Open access
PDF file
PYPavel Yudin
Pavel Yudin
AAAleksandr Petrovich Amosov
Aleksandr Petrovich Amosov
ALAleksandr Lozhkomoev
Aleksandr Lozhkomoev
DMDmitry Maidan
Dmitry Maidan
Problem. The effect of polymer coatings on the protection of steels against CO2 corrosion has been little studied, and existing standards for evaluating their adhesive strength contain contradictions in the interpretation of test results. Aim. To develop a model of changes in the adhesive strength of coatings for oilfield and tubing pipes in a CO2-containing environment for predicting their service life. Methods. Three types of polymer coatings used for the protection of oilfield and tubing pipes (tubing) were studied: a liquid non-thermosetting coating (coating 1) and two two-layer powder coatings (coatings 2 and 3). The tests were carried out using an autoclave complex. The conditions in the autoclave were the following: total system pressure 10±0.5 MPa; temperature 90±3 °С; electrolyte – sodium chloride solution in distilled water with a mass fraction of 3 %; exposure duration – 50 days. Adhesive strength was determined by the dolly pull-off method. For microscopic analysis, cross-sections of the coatings at locations of blisters were prepared, then metallographic sections were prepared. Results. After 50 days of exposure in a CO2 environment, the adhesive strength of the coatings decreased: for coating 1 – from 7.8 to 2.9 MPa, for coating 2 – from 27.1 to 10.2 MPa, for coating 3 – from 16.1 to 11.3 MPa. Coating 1 showed low initial adhesive strength values that did not meet industry standards. For coating 2, adhesion decreased in the 0–10 and 20–30 day intervals and then stabilised. For coating 3, an initial increase in adhesion was observed, followed by a decrease. Conclusions. After 50 days of exposure in a CO2 environment, the adhesive strength of coating 1 decreased by 37 % of its initial strength, of coating 2 – by 38 %, and of coating 3 – by 7 %, which recommends it for operation under similar conditions.

10 January 2026 in Powder Metallurgy аnd Functional Coatings
Verified
Journal Article
Open access
PDF file
PYP. E. Yudin
P. E. Yudin
ALAleksandr Lozhkomoev
Aleksandr Lozhkomoev
Corrosion is one of the primary causes of failure in oil and gas equipment, affecting not only its service life but also operational safety. In the Russian Federation, crude-oil production is increasingly complicated by the high water content of produced fluids, which significantly accelerates corrosion processes. The use of internal polymer coatings in pipelines partly mitigates this problem; however, the proportion of corrosion-related failures remains high. Effective protection of oil pipelines using polymer coatings requires a clear understanding of their degradation mechanisms, including under conditions that closely approximate field operation. Such understanding enables the development of effective solutions that help maintain the operating stock of oil wells in serviceable condition. This work summarizes the principal mechanisms of degradation of polymer coatings on metallic surfaces, including under exposure to aggressive environments. The key factors governing coating failure in oil pipelines are identified: diffusion and absorption of water molecules within the polymer matrix; disruption of molecular interactions in the polymer network; delamination due to loss of adhesion between the coating and the metal; interfacial corrosion; cathodic delamination; blister formation; and erosion-driven damage. The study presents results of the examination of various epoxy–novolac-based anticorrosion coatings removed from pipelines after field service and provides representative images of coatings at different degradation stages. The aim of the work was to consolidate current knowledge on the degradation mechanisms of polymer coatings on metals under diverse conditions and to refine the staged description of coating degradation in oil pipelines.