The relevance of the study is related to the need to join dissimilar copper and nickel alloys by laser direct energy and material deposition (LDED). The purpose of research is studying the distribution of elements, structure, and properties of contact zone of nickel-based super alloy and CuCr1 bronze obtained by direct energy and material deposition with preliminary formation of relief of contact surface. For the purposes of research, samples were made from UNS C18200 copper alloy CuCr1 without relief, with a relief of 0.5 mm depth, and with a relief of 1 mm depth. The Ni50Cr33W4.5Mo2.8TiAlNb (EP648) alloy powder was deposited onto the bronze samples with a micro-relief. The deposition was produced by direct injection of energy and material. The influence of interphase interaction of CuCr-chromium carbide system on the possibility of initiation of a crack in the area of carbide secretions is not significant and does not exceed 3.1% according to CIC criterion from the background level for CuCr1 (CIC = 1.54% for CuCr1-Al4C3 interface and CIC = 3.1% for CuCr1-Cr23C6 interface). An X-ray analysis revealed the presence of tensile residual macro-stresses, arising from differences in thermal expansion coefficients in the CuCr1-EP648 interface area, which may be the main cause of crack formation. Cracks are generated and run along the grain boundaries, on which traces of excretion are visible. The contact surface in the CuCr1-EP648 interface area has no visible defects, which indicates the good adhesion of materials when applying an initial layer of EP648 by LDED. The presence of a 0.5-mm micro-relief on CuCr1 has a positive effect on the strength of the connection, as it increases the surface area of the contact CuCr1-EP648 and therefore reduces the contact stress of the breakout.
1 January 2020 in Vektor nauki Tol'yattinskogo gosudarstvennogo universiteta
The formation of zinc coating on steels in the process of hot galvanizing is determined by such factors as the process temperature, holding time, the chemical composition of steel, and particularly, silicon content. In the 1940s of the XX century, R.W. Sandelin described the process of the significant acceleration of the reaction between ferrum and zinc at the silicon content in steel equal to 0.06–0.10 %. There are different methods of control of silicon reactance; however, the simplest method of control of coating thickness is the proper choice of time of product holding in the melt. The paper aims at the identifying the influence of time of holding in the melt on thickness and microstructure of the coating formed on steels with different content of silicon: S235 (Si=0.02 %), S235J0 (Si=0.04 %), S235JR (Si=0.17 %), 9MnSi5 (Si=0.6 %). To quantify silicon, the authors analyzed the chemical composition of steels using the spark spectrometry technique. The study identified that the coating thickens on steel with the course of time of holding in the melt according to the parabolic law. The most intensive growth of coating thickness with the course of time is observed on reactive steels with silicon content of 0.04 % and high-silicon steels with silicon content of 0.6 %. The reactive steel showed the significant growth of variations in thickness. The authors carried out the analysis of microstructure using the TESCAN Vega SB scanning electron microscope; the analysis showed that the growth of a coating is determined by the peculiarities of ζ-phase structure. The analysis of the Fe-Zn-Si triple diagram allowed concluding that with the silicon content of 0.04 % and 0.6 % in steel, the eutectic decomposition of fluid into ζ+η+FeSi phases’ mixture progresses in the system. This process leads to the direct contact of the melt and steel base and intensifies the interdiffusion of ferrum and zinc. As a result, the ζ-phase actively produces that leads to the rapid growth of the coating thickness.
25 December 2024 in Bulletin of the Siberian State Industrial University
INFLUENCE OF HYDROGEN ABSORPTION ON DESTRUCTION AND MECHANICAL CHARACTERISTICS OF TITANIUM ALLOY | Kudryashova | Bulletin of the Siberian State Industrial University ИССЛЕДОВАНИЕ ВЛИЯНИЯ НАВОДОРОЖИВАНИЯ НА РАЗРУШЕНИЕ И МЕХАНИЧЕСКИЕ ХАРАКТЕРИСТИКИ ТИТАНОВОГО СПЛАВА | Кудряшова, | Вестник Сибирского государственного индустриального университета