There are a number of existing models for estimating the charge states of defects in silicon. In order of increasing complexity, these are (a) the Fermi-Dirac distribution, (b) the Shockley-Last model, (c) the Shockley-Read-Hall model, and (d) the Sah-Shockley model. In this work, we demonstrate their consistency with the general occupancy ratio α, and show that this parameter can be universally applied to predict the charge states of both monovalent and multivalent deep levels, under either thermal equilibrium or steady-state conditions with carrier injection. The capture cross section ratio is shown to play an important role in determining the charge state under non-equilibrium conditions. The application of the general occupancy ratio is compared with the quasi-Fermi levels, which are sometimes used to predict the charge states in the literature, and the conditions where the latter can be a good approximation are identified. The general approach is then applied to the prediction of the temperature- and injection level-dependent charge states for the technologically important case of multivalent monatomic hydrogen, and several other key monovalent deep levels including Fe, Cr, and the boron-oxygen complex in silicon solar cells. For the case of hydrogen, we adapt the model of Herring et al., which describes the charge states of hydrogen in thermal equilibrium, and generalize it for non-equilibrium conditions via the inclusion of the general occupancy ratio, while retaining the pre-factors which make the model more complete. Based on these results, the impact of temperature and injection on the hydrogenation of the key monovalent defects, and other pairing reactions, are discussed, demonstrating that the presented model provides a rigorous methodology for understanding the impact of charge states.
It is known that the interstitial iron concentration in silicon is reduced after annealing silicon wafers coated with plasma-enhanced chemical vapour deposited (PECVD) silicon nitride films. The underlying mechanism for the significant iron reduction has remained unclear and is investigated in this work. Secondary ion mass spectrometry (SIMS) depth profiling of iron is performed on annealed iron-contaminated single-crystalline silicon wafers passivated with PECVD silicon nitride films. SIMS measurements reveal a high concentration of iron uniformly distributed in the annealed silicon nitride films. This accumulation of iron in the silicon nitride film matches the interstitial iron loss in the silicon bulk. This finding conclusively shows that the interstitial iron is gettered by the silicon nitride films during annealing over a wide temperature range from 250 °C to 900 °C, via a segregation gettering effect. Further experimental evidence is presented to support this finding. Deep-level transient spectroscopy analysis shows that no new electrically active defects are formed in the silicon bulk after annealing iron-containing silicon with silicon nitride films, confirming that the interstitial iron loss is not due to a change in the chemical structure of iron related defects in the silicon bulk. In addition, once the annealed silicon nitride films are removed, subsequent high temperature processes do not result in any reappearance of iron. Finally, the experimentally measured iron decay kinetics are shown to agree with a model of iron diffusion to the surface gettering sites, indicating a diffusion-limited iron gettering process for temperatures below 700 °C. The gettering process is found to become reaction-limited at higher temperatures.
This paper investigates the potential of three different methods-tabula rasa (TR), phosphorus diffusion gettering (PDG), and hydrogenation, for improving the carrier lifetime in n-type Czochralski-grown upgraded metallurgical-grade (UMG) silicon samples. Our results show that the lifetimes in the UMG wafers used in this study were affected by both mobile metallic impurities and as-grown oxygen precipitate nuclei. Thus, the dissolution of grown-in oxygen precipitate nuclei via TR and the removal of mobile impurities via PDG step were found to significantly improve the electronic quality of the UMG wafers. Finally, we report bulk lifetimes and 1-sun implied open-circuit voltages of the UMG wafers after boron and phosphorus diffusions, as typically applied in n-type cell fabrication.
We investigated ring defects induced by a two-step anneal in n-type Czochralski-grown silicon wafers using a combination of high spatial resolution Fourier Transform Infrared Spectroscopy (FTIR), micro-photoluminescence (PL) mapping, and micro-Raman mapping. Through FTIR measurements, we show the inhomogeneous loss in interstitial oxygen with a positive correlation with the inverse lifetime. Using high-resolution micro-PL mapping, we are able to distinguish individual recombination-active oxygen precipitates within the rings with a decreasing density from the center to the edge of the sample. The radial inhomogeneity of the oxygen precipitates is likely to be related to variations in the distribution of grown-in defects. We also demonstrate that micro-Raman mapping reveals the oxygen precipitates without the smearing effects of carrier diffusion that are present in micro-PL mapping.
This paper presents experimental studies on the formation of ring defects during high-temperature annealing in both electronic-grade and upgraded metallurgical-grade (UMG) Czochralski-grown silicon wafers. Generally, a faster onset of ring defects, or shorter incubation time, was observed in the UMG samples ([Oi] = 6.3 × 1017 cm−3) in comparison to the electronic-grade samples ([Oi] = 3.9 × 1017 cm−3) used in this work. By applying a tabula rasa (TR) treatment prior to annealing, the incubation time can be increased for both types of wafers. We show that TR temperatures above 1000 °C are necessary to effectively dissolve grown-in oxygen precipitate nuclei and limit the subsequent formation of ring defects. A 30 min TR treatment at 1000 °C resulted in the longest incubation time for both types of samples used in this work, as it achieved the best balance between precipitate nuclei dissolution and precipitate re-growth/ripening. Finally, a nitrogen ambient TR step showed a short incubation time for the formation of ring defects in comparison to an oxygen ambient TR step.