Rotary degassing is one of the most frequently used melt treatment technologies used for processing liquid aluminum alloys. Despite this, the information available about the possible effects of this method on the double oxide- and nitride film (bifilm) content, especially when using different purging gases, is quite limited. For this reason, in this study, the effects of multiple rotary degassing treatments conducted with N2 and Ar purging gases on the bifilm quantity of a casting aluminum alloy were compared. The characterization of the melt quality was realized by the computed tomographic (CT) analysis of reduced pressure test (RPT) specimens, image analysis, and scanning electron microscopy (SEM) of the fracture surfaces of K-mold samples. Based on the results, by the application of Ar as a purging gas, relatively low bifilm content can be achieved. On the other hand, while the use of N2 leads to the formation of numerous small-sized nitride bifilms, which significantly increased the pore number density inside the RPT specimens. This can be associated with the nitride formation by the chemical reaction between the liquid aluminum alloy and the N2 purging gas bubbles during the degassing treatments. Graphical abstract
30 September 2022 in Metallography, Microstructure, and Analysis
Porosity plays an important role in the properties of powder metallurgy products and castings. Nowadays, there are several methods for determining porosity: optical microscopy, computed tomography, and density measurement according to Archimedes’ principle. The aim of this study is to present the advantages and disadvantages of different porosity testing methods and the relationships between the results. With conventional metallographic methods, only two-dimensional information about pores is obtained. The accuracy of a three-dimensional CT examination is significantly affected by the resolution, the quality of the image, and the evaluation process. The porosities of aluminum (AlSi7MgCu0.5) reduced pressure test samples with different densities were determined on 3D x-ray images with the evaluation software VGStudio MAX 3.3 and on 2D section x-ray images and the optical microscope images with the image analysis software ImageJ. The effect of morphological transformation of 3D images and the role of the region of interest volume and area under examination are also discussed.
15 April 2020 in International Journal of Engineering and Management Sciences
The most common, and in fact, the most deleterious defects of aluminum casting alloys are the so-called double oxide films or bifilms, which have a central role in porosity formation, as they can easily unfurl and inflate into pores during the solidification of the alloys. Sr addition is generally used in the foundry industry for the modification of the eutectic Si phase of hypoeutectic Al-Si alloys. However, Sr microalloying usually leads to an increased pore formation tendency. As bifilms are preferred sites for pore formation, it should be expected that Sr additions have a significant effect on the number and/or the structure of double oxide films present in the melt. In this work, the relationship between Sr-concentration and the susceptibility to pore formation has been investigated through the evaluation of melt quality of melts which had different levels of Sr. The bifilm content of the melts was investigated by the analysis of K-mold specimens and X-ray computed tomography (CT) of reduced pressure test (RPT) samples. It was found that liquid alloys with a higher Sr concentration had a significantly greater tendency to pore formation, which can be explained by the presence of a larger number of bifilm defects in the liquid alloy.