H. V. Rusakova

H. V. Rusakova

Auto-generated profile, based on publicly available information

H. V. Rusakova

B. Verkin Institute for Low Temperature Physics and Engineering of the National Academy of Sciences of Ukraine , Kharkiv 61103

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 November 2021 in Materials Science and Engineering: A
Verified
Journal Article
Closed access
HRH.V. Rusakova
H.V. Rusakova
LFL.S. Fomenko
L.S. Fomenko
SSSergey Smirnov
Sergey Smirnov
APA.V. Podolskiy
A.V. Podolskiy
YSY.O. Shapovalov
Y.O. Shapovalov
ESE. Schafler
E. Schafler

1 December 2019 in Low Temperature Physics
Verified
Journal Article
Open access
PDF file
HRH. V. Rusakova
H. V. Rusakova
LFL. S. Fomenko
L. S. Fomenko
SLS. V. Lubenets
S. V. Lubenets
VNV. D. Natsik
V. D. Natsik
The microindentation of thin polystyrene plates, which is an amorphous linear thermoplastic polymer with a glass transition temperature Tg ≈ 373 K, was carried out in the 77–295 K temperature range. A decrease in the temperature from 295 K to 140 K generated a two-fold linear increase in microhardness, which is in good agreement with the temperature dependence of the forced elasticity limit of polystyrene measured by other authors during uniaxial compression deformation. At temperatures of T = 77–140 K the local deformation of polystyrene was reversible: during heating to room temperature the impressions on the sample surface disappeared completely. Partial deformation reversibility was observed upon indentation in the temperature range of 140–190 K, but at indentation temperatures T > 190 K the impressions remained. The microstrain reversibility of polystyrene in nitrogen at, and close to, 77 K is due to the effect of the adsorption-active medium on the formation of crazes (fibrillar-porous nanostructures), the glass transition temperature of which is tens of degrees below that of bulk polymer.

1 March 2020 in Low Temperature Physics
Verified
Journal Article
Open access
PDF file
HRH. V. Rusakova
H. V. Rusakova
LFL. S. Fomenko
L. S. Fomenko
SLS. V. Lubenets
S. V. Lubenets
ADA. V. Dolbin
A. V. Dolbin
NVN. A. Vinnikov
N. A. Vinnikov
ABA. V. Blyznyuk
A. V. Blyznyuk
The authors have studied the effect of small (≤ 1 wt%) additions of thermally reduced graphene oxide on the microhardness and microindentation kinetics in two types of polymers: polystyrene (i.e. thermoplastic with a glass transition temperature of Tg ≈ 373 K) and polyester resin (i.e. thermosetting plastic, Tg ≈ 300 K). The room temperature creep of nanocomposites under an indenter is described using a three-element rheological Kelvin–Voigt model. The study determines the parameters of this model and how graphene oxide (GO) affects them. In a polystyrene nanocomposite with 0.3 wt % graphene oxide, unrelaxed and relaxed elastic moduli, and the modulus characterizing high-elastic deformation, increase by 11%, 40% and 87%, respectively, as compared to the initial polystyrene; at the same time, microhardness increases by 38% and 45% for the different series of samples. The results obtained indicate that the presence of graphene oxide in the nanocomposite severely restricts the mobility of molecular segments. The addition of 0.3 wt% graphene oxide to polyester resin is accompanied by an increase in the mechanical glass transition temperature of the resin by at least 5 K. This leads to a change in the relaxation state of this polymer: while at room temperature the polyester resin behaves like an elastomer, a polyester resin nanocomposite with 0.3 wt% graphene oxide exhibits glassy properties. At room temperature, the microhardness of polyester resin-glass fabric-graphene oxide nanocomposites with a GO content of 0.5 and 1 wt% increases by 20% and 80% respectively, as compared to that of a polyester resin-glass fabric composite. The authors have obtained the temperature dependences of the microhardness of nanocomposites with a polyester matrix in the range 77–298 K, and have also identified temperature regions where the microdeformation of composites is reversible, which is associated with the formation of crazes with a lower glass transition temperature.

1 March 2022 in Low Temperature Physics
Verified
Journal Article
Closed access
PDF file
VNV. D. Natsik
V. D. Natsik
HRH. V. Rusakova
H. V. Rusakova
A molecular-kinetic model of the processes of highly elastic deformation of amorphous polymers is proposed and, on its basis, nonlinear rheological equations are obtained; these latter make it possible to describe these processes under changes of deformation conditions in a wide range: temperature, deforming stress, and strain rate. A connection of the nonlinear micromechanical model of a polymer with the classical macromechanical model of a standard linear body is established. The transitions between the structural-deformation states of a warm and frozen elastomer, as well as the effects of low-temperature deformation melting and quantum elasticity of an amorphous polymer, are discussed.

1 November 2020 in Low Temperature Physics
Verified
Journal Article
Closed access
PDF file
SDS. N. Dub
S. N. Dub
GTG. N. Tolmachova
G. N. Tolmachova
SLS. V. Lubenets
S. V. Lubenets
LFL. S. Fomenko
L. S. Fomenko
HRH. V. Rusakova
H. V. Rusakova
Elastic-plastic transition at nanoindentation of (111) plane of pure C60 fullerite single crystals was studied. The onset of plastic deformation in the contact was noted due to the plateau formation in the initial part of loading curve. The estimated stress of plasticity beginning was found to be on the order of the theoretical shear stress required for homogeneous dislocation nucleation in the ideal crystal lattice of C60. The empirical values of elastic modulus E ∼ 13.5 GPa, hardness of the ideal crystal lattice H ∼ 1.4 GPa, and hardness at different indentation loads were obtained. The hardness vs load dependence was found consistent with the model of geometrically necessary dislocations. The loading diagrams shape and the dependencies of contact pressure vs indentation depth were strongly affected by gaseous interstitial impurities (hydrogen, oxygen, nitrogen) in C60 crystal; transition stress was essentially less and plateaus formation was observed at elevated indentation loads and depths as compared with pure fullerite crystal. For crystals, saturated with hydrogen, the enhanced value of elastic modulus (∼ 20.4 GPa) and hardness (∼ 1.1 GPa) were obtained. The results acquired at room temperature for C60 with face-centered cubic lattice are important for the description of the physical-mechanical properties of simple cubic lattice phase of C60 below 260 K (S. V. Lubenets, L. S. Fomenko, V. D. Natsik, and A. V. Rusakova, Fiz. Nizk. Temp. 45, 3 (2019) [Low Temp. Phys. 45, 1 (2019)]).

1 November 2023 in Low Temperature Physics
Verified
Journal Article
Open access
PDF file
VNV. D. Natsik
V. D. Natsik
HRH. V. Rusakova
H. V. Rusakova
One of the important problems of the modern rheology of polymer materials, namely, the possibility of describing the deformation of amorphous polymers within the framework of linear rheological relationships between relative deformation and deforming stress or the need to use nonlinear rheological equations is considered. The criteria for distinguishing these approaches, namely, the determination of the corresponding critical values of the macro- and microphysical characteristics of the material and the conditions for carrying out the mechanical tests are also discussed. In particular, the difference between the influence of kinetic and thermodynamic nonlinear effects on the regularities of deformation processes of amorphous polymers in warm and frozen states was noted. The influence of nonlinear effects on the general shape and characteristics of individual stages of the “relative strain - deforming stress” diagram at deformation of polymer samples with specified values of strain rate and temperature is analyzed in detail. The results of the theoretical analysis were used for the physical interpretation of the general form and features of individual stages of the tensile test diagrams of amorphous polyimide films (V. D. Natsik, H. V. Rusakova, S. V. Lubenets, V. A. Lototskaya, and L. F. Yakovenko, Fiz. Nyzk. Temp. 49, 569 (2023) [Low Temp. Phys. 49, 521 (2023)]), empirical estimates for the rheological characteristics of this polymer were obtained.