Keiko Matsuda

Keiko Matsuda

Auto-generated profile, based on publicly available information

Keiko Matsuda

Toray Research Center, Inc., Otsu 520-8567, Japan

Research Focus & Metrics

Academic Career Length

16Years (2011-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 October 2012 in Japanese Journal of Applied Physics
Verified
Journal Article
Closed access
KMKeiko Matsuda
Keiko Matsuda
TWTakeshi Watanabe
Takeshi Watanabe
KSKoichi Sakaguchi
Koichi Sakaguchi
MYMasanobu Yoshikawa
Masanobu Yoshikawa
TDTakuya Doi
Takuya Doi
AMAtsushi Masuda
Atsushi Masuda
We used several analytical methods to identify the mechanism underlying the performance degradation in a photovoltaic (PV) module subjected to long-term (10 years) field exposure. Cloudy visual defects in this module were caused by delamination between the poly(ethylene vinyl acetate) (EVA) and antireflection coating films on the Si substrate. The delamination was considered to be caused by the formation of a segregation layer and oxidative degradation of EVA. Furthermore, it was found that sodium ions diffused from the superstrate glass into the EVA film and Si cell. We confirm that diffusion of sodium ions caused the degradation of Si cells and the superstrate glass of this module.

1 May 2011 in Applied Spectroscopy
Verified
Journal Article
Closed access
MYMasanobu Yoshikawa
Masanobu Yoshikawa
HSHirohumi Seki
Hirohumi Seki
KIKeiko Inoue
Keiko Inoue
KMKeiko Matsuda
Keiko Matsuda
YTYusaku Tanahashi
Yusaku Tanahashi
TKTsunenobu Kimoto
Tsunenobu Kimoto
We used Fourier transform infrared (FT-IR) spectroscopy to characterize silicon dioxide (SiO(2)) films on a 4H-SiC(0001) Si face. We found that the peak frequency of the transverse optical (TO) phonon in SiO(2) films grown on a 4H-SiC substrate agrees well with that in SiO(2) films grown on a Si substrate, whereas the peak frequency of the longitudinal optical (LO) phonon in SiO(2) films on a 4H-SiC substrate is red-shifted by approximately 50 cm(-1) relative to that in SiO(2) films on a Si substrate. We concluded that this red-shift of the LO phonon is mainly caused by a change in inhomogeneity due to a decrease in density in the SiO(2) films. Furthermore, cathodoluminescence (CL) spectroscopy results indicated that the channel mobility of the SiC metal-oxide-semiconductor field-effect transistor (MOSFET) decreases roughly in proportion to the increase in the intensity of the CL peak at 460 and 490 nm, which is attributed to the increase in the number of oxygen vacancy centers (OVCs). FT-IR and CL spectroscopies provide us with a large amount of data on OVCs in the SiO(2) films on a 4H-SiC substrate.