Strain and composition distributions within wurtzite InGaN/GaN layers are investigated by high-resolution reciprocal space mapping (RSM). We illustrate the potential of RSM to detect composition and strain gradients independently. This information is extracted from the elongation of broadened reciprocal lattice points (RLP) in asymmetric x-ray reflections. Three InxGa1−xN/GaN (nominal x=0.25) samples with layer thickness of 60, 120, and 240 nm, were grown in a commercial metal-organic chemical vapor deposition reactor. The RSMs around the (105) reflection show that the strain profile is nonuniform over depth in InGaN. The directions of “pure” strain relaxation in the reciprocal space, for a given In content (isocomposition lines), are calculated based on elastic theory. Comparison between these directions and measured distributions of the RLP shows that the relaxation process does not follow a specific isocomposition line. The In mole fraction (x) increases as the films relax. At the start of growth all the films have x∼0.2 and are coherent to GaN. As they relax, x progressively increases towards the nominal value (0.25). Compositional gradients along the growth direction extracted from the RSM analysis are confirmed by complementary Rutherford backscattering measurements.
1 November 2000 in Surface and Coatings Technology
A depth-resolved study of the optical and structural properties of wurtzite InGaN/GaN bilayers grown by metallorganic chemical vapor deposition on sapphire substrates is reported. Depth-resolved cathodoluminescence (CL) and Rutherford backscattering spectrometry (RBS) were used to gain an insight into the compositional profile of a 75-nm thick InGaN epilayer in the direction of growth. CL acquired at increasing electron energies reveals a peak shift of about 25 meV to the blue when the electron beam energy is increased from 0.5 to ∼7 keV, and shows a small shift to lower energies between ∼7 and 9 keV. For higher accelerating voltages the emission energy peak remains constant. This behavior can be well accounted for by a linear variation of In content over depth. Such an interpretation conforms to the In/Ga profile derived from RBS, where a linear decrease of the In mole fraction from the near surface (∼0.20) down to the near GaN/InGaN interface (∼0.14) region fits the random spectra very well. Furthermore, by measuring the tetragonal distortion at different depths, using RBS/channeling, it is shown that regions of higher In content also appear to be more relaxed. This result suggests that strain hinders the incorporation of In atoms in the InGaN lattice, and is the driving force for the compositional pulling effect in InGaN films.