1 August 2006 in American Journal of Orthodontics and Dentofacial Orthopedics
Verified
Journal Article
Closed access
AAAyca Arman
Ayca Arman
SCS. Burcak Cehreli
S. Burcak Cehreli
EOEmre Ozel
Emre Ozel
NANeslihan Arhun
Neslihan Arhun
AÇAlev Çetinşahin
Alev Çetinşahin
MSMubin Soyman
Mubin Soyman

1 March 2011 in Operative Dentistry
Verified
Journal Article
Closed access
ÖMÖ Malkondu
Ö Malkondu
HYH Yurdagüven
H Yurdagüven
ESEc Say
Ec Say
Ender KazazogluEnder Kazazoglu
Ender Kazazoglu
MSM Soyman
M Soyman
Clinical Relevance: High-concentration carbamide peroxide containing home bleaching may cause a varying influence on the microhardness of esthetic restorative materials.

1 March 2009 in Operative Dentistry
Verified
Journal Article
Closed access
EOE. Ozel
E. Ozel
MSM. Soyman
M. Soyman
SUMMARY: This study evaluated the effects of fiber nets and application techniques and flowable composites as a liner on microleakage and the effects of fiber nets on polymerization shrinkage in Class II MOD cavities. Standard MOD cavities were performed in 80 extracted third molars. The teeth were randomly divided into eight groups (n=10). Group 1: Filtek Supreme XT (bulk technique) (FSB); Group 2: Filtek Supreme XT (incremental technique) (FSI); Group 3: Filtek Supreme XT Flow (FS Flow)+FSB; Group 4: FS Flow+FSI; Group 5: FS Flow+Ribbond (R)+FSB; Group 6: FS Flow+R+FSI; Group 7: FS Flow+everStick NET (E)+FSB; Group 8: FS Flow+(E)+FSI. All the teeth were then immersed in 0.5% basic fuchsin solution for 24 hours after thermocycling for 1000 cycles (5°C and 55°C). The teeth were sectioned longitudinally and observed under a stereomicroscope. In order to determine the polymerization shrinkage, another study was designed. In Group A, composite was applied as a bulk. In Group B, the resin composite was divided into two parts and Ribbond fiber was placed in the middle of the mass. In Group C, everStick NET fiber was placed inside the composite, as in Group B. Statistical analysis were performed by using one-way ANOVA and Tukey HSD tests for both microleakage and polymerization shrinkage (p<0.05). Less microleakage was observed in groups where composites were applied by the incremental technique compared with those where the bulk technique was used (p<0.05). The groups that used flowable composites showed significantly lower microleakage (p<0.05). In groups where fiber nets were used, a significant decrease was determined in terms of microleakage (p<0.05). Groups with fiber nets exhibited lower polymerization shrinkage (p<0.05). Fiber nets decreased both microleakage and polymerization shrinkage. The incremental technique is an effective method for Class II composite restorations.

1 April 2006 in Journal of Dentistry
Verified
Journal Article
Closed access
ESEsra Can Say
Esra Can Say
MNMasatoshi Nakajima
Masatoshi Nakajima
PSPisol Senawongse
Pisol Senawongse
MSMübin Soyman
Mübin Soyman
FÖFüsun Özer
Füsun Özer
JTJunji Tagami
Junji Tagami

1 January 2012 in European Journal of Dentistry
Verified
Journal Article
Open access
PDF file
HYHaktan Yurdaguven
Haktan Yurdaguven
AAArzu Aykor
Arzu Aykor
EOEmre Ozel
Emre Ozel
HSHilmi Sabuncu
Hilmi Sabuncu
MSMubin Soyman
Mubin Soyman
Objective: To investigate the effect of a prophylaxis paste on surface roughness of different composites, enamel, dentin and porcelain surfaces.Methods: Three different composites (FiltekZ250/Group1, Filtek Supreme XT/Group2, Premise/ Group3), enamel/Group4, dentin/Group5 and porcelain/Group6 samples were used in this study. All specimens were prepared flat by SiC discs and polished with a diamond polishing paste. The surface roughness measurements were determined with a profilometer after polishing (initial surface roughness). Prophylaxis paste was applied to the samples for 12 seconds, renewing every 6 seconds. After cleaning the samples, roughness values were measured again. Data were analyzed by Kruskal Wallis and Dunn’s multiple comparison test. Wilcoxon test was performed for the comparison of the initial and final surface roughness values (P<.05). The results were evaluated within the P<.05 confidence level.Results: The mean %SMHC was:C=77.27%, CL= 72.45%, SL=78.43%, G=66.65% and P=67.95%. Comparing the %SMHC promoted by 5 soft drinks, SL = C > CL > P = G (P<.05). There was not significant correlation between %SMHC and the other variables tested for the five drinks (P>>.05)Results: The initial and final surface roughness values (μm) were determined as follows: Group1: 0.039±0.009 and 0.157±0.018, Group2: 0.023±0.005 and 0.145±0.027, Group3: 0.028±0.008 and 0.109±0.012, Group4: 0.024±0.006 and 0.071±0.015, Group5: 0.030±0.007 and 0.143±0.029, Group6: 0.024±0.006 and 0.064±0.014. Significant difference was determined between the initial and final values for all groups.Conclusions: Composite and dentin surfaces were more affected by the application of prophylaxis paste than enamel and porcelain surfaces. The prophylaxis paste increased the surface roughness of all groups, but did not reach the bacterial retention roughness rate of 0.2μm. (Eur J Dent 2012;6:1-8)

1 January 2004 in Dental Materials Journal
Verified
Journal Article
Closed access
PDF file
MEMustafa Ersoy
Mustafa Ersoy
ACArzu Civelek
Arzu Civelek
ELEstelle L'HOtelier
Estelle L'HOtelier
ESEsra Can Say
Esra Can Say
MSMubin Soyman
Mubin Soyman
The purpose of this study was to determine the flexural strength (FS), flexural modulus (FM), depth of cure (DC), polymerization shrinkage (PS), and microhardness (VH) of the following composites: • Two packable composites - Filtek P-60 and Solitaire 2; One ion-releasing composite - Ariston AT; and • Two hybrid composites - Charisma and Filtek Z-250. Data of the different tests conducted were obtained as follows: • FS and FM data were determined with a universal-testing machine; • Polymerization shrinkage was determined using the apparatus of Watts and Cash; • Depth of cure was measured with a micrometer (Mitotuyo, UK); and • Microhardness was measured with a Shimadzu Microhardness tester (500g, 15 seconds). All data of the different tests were statistically analyzed by one-way variance analysis (ANOVA), which yielded the following results: • Filtek Z-250 showed the statistically highest flexural strength and modulus values. • Solitaire 2 exhibited the highest shrinkage, while the volumetric shrinkage results of Filtek Z-250 and Filtek P-60 ranked the lowest. • For depth of cure, there were no statistically significant differences among all materials tested (pAriston AT=Solitaire 2=Charisma.