Due to the ever-increasing abundance of discarded by-products, it is imperative to develop innovative engineering applications of waste materials, to manage the capacity of landfills. The disposal and landfilling issues associated with tyre waste have necessitated Australian authorities to find innovative applications of tyre waste in pavement construction. In this research, to examine the efficiency of tyre-derived aggregates (TDAs) as a replacement material for quarry aggregates in pavement subbase applications, a series of repeated load triaxial (RLT) tests and wheel-tracker (WT) tests were undertaken on specimens made of proportioned recycled concrete aggregate (RCA) blended with small-sized TDA (TDA-S) and medium-sized TDA (TDA-M), thus merging these two waste materials into a valued pavement-construction material. The results from the RLT and WT tests confirmed that TDA–RCA blends are a suitable alternative for pavement base/subbase materials. Compared with TDA-S, TDA-M resulted in a lower rutting deformation and permanent deformation in WT and RLT tests, respectively. The resilient modulus (M r) of the RCA + TDA-M mix was also found to be higher than that of the RCA + TDA-S mix, and it was almost comparable with the M r of the control RCA.
Stone columns develop their load-bearing capacity from the circumferential confinement offered by the surrounding soils. In highly plastic soils, the circumferential confinement provided by the surrounding soft soils may not be sufficient to develop the required bearing capacity. Meanwhile, the ground improvement industry has been keen to explore substitution backfill materials due to the depletion of natural aggregate resources typically used to construct stone columns. This research investigated the viability of using recycled concrete aggregate (RCA) and recycled aluminum salt slag (RASS), stabilized with alkali-activated fly ash (FA), slag (S) and a binary precursor (FA+S), as a novel semi-rigid inclusion column system for ground improvement of soft soils. The effect of the RCA/RASS ratios, additive types and dosages along with different curing conditions on the unconfined compressive strength (UCS) of geopolymer-stabilized mixtures, were evaluated. Various reinforcing mechanisms were suggested through the microstructure characterization of the mixtures. In addition, the permanent deformation responses of mixtures under cyclic loading were studied using repeated load triaxial (RLT) tests that simulate the cyclic moving traffic loads imposed on the stone columns system. The results demonstrated that increasing the RASS contents resulted in a subsequent decline in the UCS of the mixtures. Increasing the additive dosages on the other hand in general led to higher strengths. The effects of both curing duration and temperature were found to play a vital role in the strength development of the mixtures. Furthermore, 100RCA stabilized by as low as 5% alkali-activated FA, S or (FA+S), met the minimum UCS requirement of 1.034 MPa for ground improvement. The highest reduction in permanent strains of 87.3% was recorded for the stabilized 100RCA + 10%(FA+S) mixture compared to the unbound 100RCA (control group). The practical implications of the findings were also discussed in detail throughout the paper.
Foamed bitumen stabilisation (FBS) is widely used to enhance durability, moisture resistance, and road flexibility while reducing cracking. Addressing knowledge gaps in its application with recycled materials can expand their usage in road construction. This study focused on stabilising mixes of 50% recycled concrete aggregate (RCA) and 50% fine recycled glass (RG) using foamed bitumen (FB). Recycled toner aggregate (RTA) and geopolymers derived from ground granulated blast furnace slag (S) and fly ash (FA) were evaluated as potential alternatives to conventional secondary binders, such as Portland cement for FBS of recycled material blends. To assess the performance of RTA, a fixed 3% FB dosage was combined with varying RTA amounts (1%–4%). Geopolymers including FA, S, and (FA + S) at dosages of 10%, 20%, and 30% by mass of RCA and RG blend were tested alongside 3% FB for their stabilising effectiveness. FB-stabilised samples with RTA initially failed the indirect tensile modulus tests, but their performance improved significantly after extended curing. The blend incorporating geopolymers, RCA + RG + 3% FB + 20% (FA + S), met local road authority standards. These results demonstrate the potential of sustainable secondary binders for the stabilisation of RCA and RG mixtures in road construction.