Additive manufacturing enables architectured porous material design, but 3D-CAD modelling of these materials is prohibitively computationally expensive. This bottleneck can be removed using a line-based representation of porous materials instead, with strut thickness controlled by the supplied laser energy. This study investigated how laser energy and scan strategy affects strut thickness and mechanical strength of porous materials. Specimens were manufactured using varying laser parameters, 3 scan strategies (Contour, Points, Pulsing), 2 porous architectures and 2 materials (Titanium, Stainless Steel), with strut thickness, density, modulus, mechanical strength and build time measured. Struts could be built successfully as low as 15° with a minimum diameter of 0.13 mm. Strut thickness was linearly related to the specific enthalpy delivered by the laser to the melt-pool. For a given stiffness, Titanium specimens built at low power/slow speed had a 10% higher strength than those built at high power/fast speed. The opposite was found in Stainless Steel. As specimen stiffness increased, the Contour Strategy produced samples with the highest strength:stiffness and strength:weight ratio. The Points strategy offered the fastest build time, 20% and 100% faster than the Contour and Pulsing strategies, respectively. This work highlights the importance of optimising build parameters to maximize mechanical performance
An increasing volume of work supports utilising the mechanobiology of bone for bone ingrowth into a porous scaffold. However, typically during in vivo testing of implants, the mechanical properties of the bone being replaced are not quantified. Consequently there remains inconsistencies in the literature regarding ‘optimum’ pore size and porosity for bone ingrowth. It is also difficult to compare ingrowth results between studies and to translate in vivo animal testing to human subjects without understanding the mechanical environment.
This study explored the regenerative osteogenic response in the distal femur of sheep using scaffolds having stiffness values within, and above and below, the range of trabecular bone apparent modulus. Scaffolds 3D-printed from stiff titanium and compliant polyamide were implanted into a cylindrical metaphyseal defect 15 × 15 mm. After six weeks, bone ingrowth varied between 7 and 21% of the scaffold pore volume and this was generally inversely proportional to scaffold stiffness. The individual reparative response considerably varied among the animals, which could be divided into weak and strong responders. Notably, bone regeneration specifically within the interior of the scaffold was inversely proportional to scaffold stiffness and was strain-driven in strongly-responding animals. Conversely, bone regeneration at the periphery of the defect was injury-driven and equal in all scaffolds and in all strongly- and weakly-responding animals. The observation of the strain-driven response in some, but not all, animals highlights that scaffold compliance is desirable for triggering host bone regeneration, but scaffold permanence is important for the load-bearing, structural role of the bone-replacing device. Indeed, scaffolds may benefit from being nonresorbable and mechanically reliable for those unforeseeable cases of weakly responding recipients.