1 April 2002 in Japanese Journal of Applied Physics
Aligned carbon nanotube arrays have been grown on Si substrates in methanol by using a hot-substrate method. Samples were grown in a glass chamber equipped with a function in which methanol and ethanol vapors were condensed by means of water-cooling. Si substrates with a thin Fe film were electrically heated to 930°C in liquid methanol. Hollow mutiwalled carbon nanotubes standing well on the Si substrates were obtained with external diameters ranging from 13 to 26 nm and lengths up to 20 µm, with the ratio of tube radius to the thickness of tube shells ranging from 1.7 to 2.1. The top ends of the nanotubes were closed with nearly seamless caps. The mechanism of nanotube growth is a catalytic process at the substrate surface under thermal non-equilibrium.
24 March 1997 in Applied Physics Letters
We have characterized bias-assisted chemical vapor deposition diamond using the nondestructive technique of confocal Raman spectroscopy to investigate the interfacial structures and the variation in structure and quality with depth. The spectral depth profiles of oriented diamond showed that a band centered at 1210 cm−1 and the diamond peak at 1332 cm−1 coexisted at the interface between the oriented diamond and Si substrate. The relative intensity of the 1210 cm−1 band compared to that of the diamond peak varied with depth. The intensity of the band decreased and that of the diamond peak increased from the interface to the diamond surface. The quality of the oriented diamond improved with the growth time. In contrast, for the case of a randomly oriented diamond, a band centered at 1550 cm−1 was observed, the diamond peak was shifted between −6 and 6 cm−1 from the single crystal diamond peak at 1332.5 cm−1, and the spectral profile did not change with depth. No band at 1210 cm−1 was seen in this case. We conclude that a nondiamond phase with a Raman band at 1210 cm−1 and a diamond phase coexist at the interface between the oriented diamond and the Si substrate, and that this 1210 cm−1 phase is therefore a characteristic feature of the nature of the diamond-substrate bonding in oriented films.
15 April 1999 in Physical Review B
The structure of the hydrogen terminated, reconstructed diamond (100) surface has been investigated by low-energy electron-diffraction (LEED) intensity versus energy measurements in combination with tensor LEED calculations. It has been found that the surface corresponds to the formation of symmetric dimers on the top C layer, with a dimer length of 1.60 Å. The top layer shows slight inward relaxation; the interlayer spacing between the first and second C layers reduces to 0.81 Å, which corresponds to an ∼7% contraction compared to the bulk value. The structural details of the first four carbon layers have been determined and are compared to those given by theoretical calculations.
2 November 1998 in Applied Physics Letters
The use of oxygen in improving diamond quality has been investigated by comparing two (111) homoepitaxial diamond films deposited with and mixtures by microwave assisted chemical vapor deposition. The (111) diamond deposited using a mixture showed surface cracks due to the presence of nondiamond phases as well as a significant amount of hydrogen and silicon impurities. The (111) diamond deposited using a mixture showed an absence of hydrogen and silicon impurities and nondiamond phases, and exhibited a flat surface. The addition of oxygen is one of the suitable methods to produce high-quality (111) homoepitaxial diamond.
6 December 2021 in RSC Advances
The development of efficient fuel cells greatly promotes reducing the consumption of fossil energy, and it is crucial to enhance the platinum (Pt) catalytic activity by optimizing both the nanoparticle size and support effect. In this study, we generate a smaller and uniform size of naked Pt nanocluster (NC) catalysts via a dry process in the gas phase, and using the direct powder embedded trapping method, the Pt NCs are spatioselectively supported on Marimo carbon (MC) that comprises a high density of carbon nanofilaments. At a minimum Pt loading of 0.05 mgPt cm−2 for both the anode and cathode in a single cell configuration, a membrane-electrode assembly (MEA) formed by the dry-deposition Pt-NC(d)/MC exhibits superior power density (rated) of 0.105 gPt kW−1 at a current density of 1.2 A cm−2, which is better output power density than the conventional MEA formed by Pt catalysts via a wet process. The origin of the improved performance is investigated using transmission electron microscopy; dry-deposition Pt catalysts that are monodispersely loaded on the outer surface of MC can facilitate not only the gas reaction but also leaving the generated water. The present results demonstrate that the dry deposition of Pt NCs on MC can be used as a scalable catalyst synthesis method to reduce the Pt loading.