The activation process of Zr, ZrVHf and TiZrV non-evaporative getter (NEG) thin films, prepared by direct current magnetron sputtering, is investigated by in situ synchrotron radiation photoemission spectroscopy. The activation temperatures of Zr and ZrVHf films are found to be 300 °C and 200 °C, respectively, and the activation temperature of TiZrV film is 120 °C—the lowest activation temperature reported on TiZrV. As the heating temperature increases, the transformation of metal-C bond follows the orders of V–C, Ti–C, Zr–C, Hf–C. It is found that the order of reduction difficulty of the same element oxides, that is, Zr oxide and V oxide in different films follows Zr film > ZrVHf film > TiZrV film. The order of difficulty in the reduction of oxides in the same alloy NEG films follows HfO2 > ZrO2 > TiO2 > V2O5. We propose that the above phenomena can be explained by interstitial diffusion, grain boundary diffusion of residual gas atoms and grain boundary precipitation of V and Ti in the solid solution of the NEG films.
Non-evaporable getter (NEG) films are widely used in high vacuum technologies and have played a critical role in applications requiring ultrahigh vacuum conditions, such as accelerator vacuum systems. The passivation layers on the film surface due to air exposure generally require thermal vacuum activation. This research aims to elucidate the key factor in the activation of TiZrV NEG films from the perspective of atomic-scale microstructures. The characteristics of film element distributions, morphologies, and crystalline states before and after activation were investigated by energy dispersive spectroscopy, scanning electron microscopy, and grazing incidence x-ray diffraction. In situ x-ray photoelectron spectroscopy was used to detect compositional variations in the film surface layer at different activation temperatures. According to the analysis, from an atomic-scale perspective, the easily activated structures would degrade in activation performance when surrounded by structures that are difficult to activate. During activation, the activated structures tend to act as channels for foreign atoms until the surrounding structures are fully activated. Hydroxyl and carbonyl groups are generally easier to activate than hydrocarbons and surface carbides, but even groups of the same type vary greatly in activation difficulty due to the differences in atomic-scale microstructures on the film surface. These findings provide valuable insight into the activation of NEG films and may be beneficial in the design of novel NEG films with excellent activation performance.