23 February 2011 in Physical Review Letters
We report the direct observation of surface magnetization domains of the magnetoelectric using photoemission electron microscopy with magnetic circular dichroism contrast and magnetic force microscopy. The domain pattern is strongly affected by the applied electric field conditions. Zero-field cooling results in an equal representation of the two domain types, while electric-field cooling selects one dominant domain type. These observations confirm the existence of surface magnetization, required by symmetry in magnetoelectric antiferromagnets.
4 May 2021 in Materials Horizons
Crystal structure without distortion for orthorhombic SrIrO 3 (left) and the room temperature in-plane band structure of SrIrO 3 (001) thin film (right). Here, the green, orange, and blue circles represent Sr, Ir, and O, respectively.
17 May 2023 in Journal of Applied Physics
NiCo2O4 (NCO) films grown on MgAl2O4 (001) substrates have been studied using magnetometry and x-ray magnetic circular dichroism based on x-ray absorption spectroscopy and spin-polarized inverse photoemission spectroscopy with various thicknesses down to 1.6 nm. The magnetic behavior can be understood in terms of a layer of optimal NCO and an interfacial layer (1.2 ± 0.1 nm), with a small canting of magnetization at the surface. The thickness dependence of the optimal layer can be described by the finite-scaling theory with a critical exponent consistent with the high perpendicular magnetic anisotropy. The interfacial layer couples antiferromagnetically to the optimal layer, generating exchange-spring styled magnetic hysteresis in the thinnest films. The non-optimal and measurement-speed-dependent magnetic properties of the interfacial layer suggest substantial interfacial diffusion.
1 June 2022 in Physica E: Low-dimensional Systems and Nanostructures
24 August 2020 in Journal of Physics: Condensed Matter
The band structures of the transition metal dichalcogenides (TMD's) 2H-MoS 2 (0001) and 2H-WSe 2 (0001), before and after palladium adsorption, were investigated through angle-resolved photoemission. Palladium adsorption on 2H-MoS 2 (0001) is seen to result in very different band shifts than seen for palladium on 2H-WSe 2 (0001). The angle resolved photoemission results of palladium adsorbed on WSe 2 (0001) indicate that palladium accepts electron density from substrate. The resulting band shift will lead to a decrease in the barriers to the hole injection. The opposite band shifts occur upon palladium adsorption between 2H-MoS 2 (0001). The overall trend is consistent with the deposition of other metals deposited on TMD's, except that for palladium adsorption on MoS 2 (0001), there is an increase in the MoS 2 (0001) substrate band gap with palladium adsorption, as is evident from the combination of photoemission and inverse photoemission.
12 April 2023 in Journal of Physics: Condensed Matter
While induced spin polarization of a palladium (Pd) overlayer on antiferromagnetic and magneto-electric Cr2O3(0001) is possible because of the boundary polarization at the Cr2O3(0001), in the single domain state, the Pd thin film appears to be ferromagnetic on its own, likely as a result of strain. In the conduction band, we find the experimental evidence of ferromagnetic spin polarized in Pd thin films on a Cr2O3(0001) single crystal, especially in the thin limit, Pd thickness of around 1–4 nm. Indeed there is significant spin polarization in 10 Å thick Pd films on Cr2O3(0001) at 310 K, i.e. above the Néel temperature of bulk Cr2O3. While Cr2O3(0001) has surface moments that tend to align along the surface normal, for Pd on Cr2O3, the spin polarization contains an in-plane component. Strain in the Pd adlayer on Cr2O3(0001) appears correlated to the spin polarization measured in spin polarized inverse photoemission spectroscopy. Further evidence for magnetization of Pd on Cr2O3 is provided by measurement of the exchange bias fields in Cr2O3/Pd(buffer)/[Co/Pd]
n
exchange bias systems. The magnitude of the exchange bias field is, over a wide temperature range, virtually unaffected by the Pd thickness variation between 1 and 2 nm.