In this paper a bump-less process is introduced in order to further scale down the pitch of microbumps. Electrical resistance measurement, Cross section SEM and mechanical characterizations show successful 3D stacking using proposed method.
19 February 2024 in Japanese Journal of Applied Physics
We investigated chemical mechanical polishing (CMP) of indium, with the goal of obtaining indium bond pads for later cryo-3D integration of quantum computing-related chips, through bonding between these bond pads and indium bumps. Higher removal rates were obtained with soft CMP pads than with hard pads. The latter led to deep scratching, while this effect was much more limited for soft pad CMP. On patterned wafers, indium is cleared well in structured areas using soft pad CMP, leading to relatively high-quality indium surfaces inside bond pads, although corrosion might be of some concern. Pattern density uniformity was an important factor for within-die deviation in indium clearing time. Dishing was much more limited than in earlier work on indium polishing, while surface roughness was also found to be relatively limited. The obtained indium damascene bond pads may be suitable for 3D die-to-die and wafer-to-wafer bonding through indium pad-to-bump bonding.
21 July 2025 in IEEE Journal on Emerging and Selected Topics in Circuits and Systems
The increasing demand for higher functional density in microelectronics necessitates the miniaturization of interconnects in 3D integration, which presents challenges in processing and reliability. During fabrication and service life, interconnect microbumps remain in a non-equilibrium state, leading to interfacial reactions and atomic diffusion that drive intermetallic compounds (IMCs) growth and phase transformations, impacting the electrical, thermal, and mechanical properties, and affecting long-term reliability. With global restrictions on Pb-based solders, indium (In) has emerged as a viable low-melting-point alternative, especially for temperature-sensitive packaging. Understanding IMCs kinetics in In-based systems is essential for optimizing reliability. This study investigates the kinetics and phase transformation of IMCs in Ni/In and Cu/In systems under solid-state aging conditions using an in-situ resistance measurement technique. The approach overcomes the limitations of traditional scanning electron microscopy (SEM)-based analysis by enabling continuous monitoring of IMCs growth. The Ni/In system forms Ni₃In₇ through a reaction-controlled mechanism with an activation energy of 108 ± 30 kJ/mol. In the Cu/In system, CuIn₂ is formed at room temperature that undergoes a phase transformation to Cu₁₁In₉ via a peritectoid reaction above 107.5 °C of iso-thermal aging. The transformation shifts from a reaction-diffusion mixed controlled regime at 110 °C (n ≈ 0.73) to diffusion control between 120-140 °C (n ≈ 0.45–0.62), and possibly to grain-boundary diffusion at 150 °C (n ≈ 0.19). The activation energy for CuIn₂ → Cu₁₁In₉ transformation is 196 ± 82 kJ/mol, indicating a higher energy barrier. These findings contribute to the development of low-temperature bonding techniques and fine-pitch interconnect optimization for future microelectronics packaging.
4 November 2025 in IEEE Transactions on Components, Packaging and Manufacturing Technology
This paper explores the challenges of microbump pitch scaling down to 5 μm for chiplet applications, including TCB tool alignment accuracy, fabrication process limitations, CTE mismatch, metal oxide reduction, and reliability concerns for die to wafer bonding. An approach called embedded bumps together with fluxless TCB are introduced to mitigate the challenges. Additionally, it discusses qubit, interposer and CMOS chips integration in 2.5D chiplet and 3D architectures for cold and quantum computing applications, where indium is used as the solder metal where successful bonding results for 20 μm pitch indium bumps are shown.