The expanded austenite γN can be produced in austenitic stainless steels by plasma nitriding, carburizing or nitrocarburizing at low temperatures. This metastable phase presents higher hardness and toughness if compared with traditional nitride layers whilst also maintaining the corrosion resistance. However, the application of plasmas composed by both nitrogen and carbon is technologically recent and the effect of such process on the microstructure and properties of the nitrocarburized layers is still under investigation. In this study, samples of UNS S31254 superaustenitic stainless steel were produced by plasma nitriding and nitrocarburizing at 400°C, 450°C and 500°C for 5h. The plasma treated samples were observed by optical and transmission electron microscopy and also analyzed by X-ray diffraction. The thickness of the layers increased with temperature and the nitrocarburized layers were thicker than nitrided at a given temperature. The presence of expanded austenite was confirmed by X-ray diffraction through its characteristic anomalous shift on the diffracted peaks related to the austenite. Nitride formation on samples produced at 400°C was only identified by transmission electron microscopy where fine rounded particles with 10–15nm size revealed reflections consistent with the CrN cubic chromium nitride. The estimated lattice parameter from the expanded austenite ranged from 0.38 to 0.41nm depending on the employed {hkl} reflection which was found to be 6–11% larger than the untreated austenite lattice parameter
1 March 2012 in Surface Engineering
Pack chromising treatment is an environmentally friendly alternative to hard chromium to form wear and corrosion resistant surface layers. In this work, samples of AISI 1060 steel were pack chromised for 6 and 9 h at 1000 and 1050°C using different activator concentrations. Wear tests were performed in dry conditions and corrosion tests in natural sea water for the pack chromised samples and hard chromium. Pack chromising yielded the formation of layers with high chromium concentrations, high hardness and wear resistance. Increasing activator concentration causes no significant change on the morphology and thickness of the layers. The layers produced at 1050°C yielded only a (Cr,Fe)2N1−x phase, and those obtained at 1000°C are composed of a carbide mixture with (Cr,Fe)2N1−x. The sample treated at 1050°C for 9 h resulted in an optimum condition by means of better wear resistance and corrosion properties, which were close to that exhibited by the hard chrome, indicating that pack chromising is a promising alternative.