The solid solutions of the (1-x)Na[ ]Bi[ ]TiO3-xNa[ ]K[ ]NbO3 system were produced by the conventional ceramic technology using mechanical activation of the synthesized product. It was found that in the (1-x)Na[ ]Bi[ ]TiO3-xNa[ ]K[ ]NbO3 system at room temperature, a number of morphotropic phase transitions occur: rhombohedral → cubic → tetragonal → monoclinic phases. The introduction of a small amount of Na[ ]K[ ]NbO3 leads to an increase in the temperature stability of the dielectric properties of ceramics. A change in the relaxor properties of the solid solutions of the (1-x)Na[ ]Bi[ ]TiO3-xNa[ ]K[ ]NbO3 system was shown. The increase in energy density and energy efficiency was found at additive 10[ ]mol.% of Na[ ]K[ ]NbO3.
Pure and superstoichiometric modified by 2[ ]wt.% Bi2O3 and 2[ ]wt.% manganese oxide (Mn2O3) ceramic samples of the binary system 0.71BiFeO3-0.29BaTiO3 were fabricated using conventional ceramic technology by double solid-phase synthesis with following sintering. Mechanical activation of synthesized powders was carried out at the stage of manufacturing press powders prepared for sintering. X-ray analysis at room temperature showed that all studied ceramics have pseudo-cubic symmetry. Grain morphology, dielectric and piezoelectric properties of selected solid solutions were investigated. The modification increased the homogeneity of the material, dielectric constant and piezomodulus [ ] and also resulted in a decrease in the dielectric loss tangent. The highest piezoelectric coefficient [ ] [ ]pC/N was obtained. Dielectric characteristics of ceramics revealed ferroelectric relaxor behavior and region of diffuse phase transition from the paraelectric to ferroelectric phase in the temperature range of 740–770[ ]K.
Barium strontium niobate films have been grown on MgO(001) substrates by single-step rf cathode sputtering of a ceramic target with the stoichiometric composition Sr0.5Ba0.5Nb2O6 in an oxygen atmosphere under various conditions (at different substrate biases). It has been shown that, depending on its polarity, the substrate bias either increases or reduces the flux of structure-forming elements to the substrate and, as a consequence, changes the growth rate, without impairing the surface morphology or surface perfection of the film or producing impurity phases. The mechanisms underlying the observed general relationships are discussed.