Utilizing reactive DC magnetron sputtering method, TiN coatings were deposited on the silicon substrates at different nitrogen flows and powers. A study of the X-ray phase composition of the coatings was carried out. The stoichiometric composition of the coatings was determined using energy dispersive x-ray spectroscopy. The structure of the surface, cross-section, and thickness of the coatings were determined using scanning electron (SEM) and atomic force microscopy (AFM). A significant change in the surface structure of TiN coatings was established with changes in deposition power and nitrogen flow. SEM images of cross-sections of all coated samples showed that the formation of coatings occurs in the form of a columnar structure with a perpendicular orientation relative to the silicon substrate. The mechanical properties (elastic modulus E and microhardness H) of TiN coatings of the first group demonstrate a maximum at a nitrogen flow of 3 sccm and are 184 ± 11 GPa and 15.7 ± 1.3 GPa, respectively. In the second group, the values of E and H increase due to a decrease in the size of the structural elements of the coating (grains and crystallites). In the third group, E and H decrease. Microtribological tests were carried out in 4 stages: at a constant load, multi-cycle for 10 and 100 cycles, and with increasing load. The coefficient of friction (CoF) and specific volumetric wear ω depend on the roughness, topology, and mechanical properties of the resulting coatings. Fracture toughness was determined using nanoscratch and depends on the mechanical properties of TiN coatings. Within each group, coatings with the best mechanical and microtribological properties were described: in the first group—TiN coating at 3 sccm (with (29.6 ± 0.1) at.% N), in the second group—TiN coating at 2 sccm (with (40.8 ± 0.2) at.% N), and in the third group—TiN coating at 1 sccm (c (37.3 ± 0.2) at.% N).
Relaxor ferroelectric lead scandium niobate Pb2ScNbO6(PSN) ceramics was obtained by solidstate synthesis and a modified ceramic technology, whereby the sintering stage was preceded by...
The Pb(Zr0.56Ti0.44)O3 (PZT) ceramics was subjected to a pressure-induced activation at 320 MPa in a Bridgman anvil, where a load pressure was combined with a shear deformation. The induced changes in the linear and angular parameters of a unit cell, in the ratio of coexisting rhombohedral (R3m) and tetragonal (P4mm) phases as well as in the dielectric properties were analyzed.
Polycrystalline multiferroic PbFe0.5Nb0.5O3 (PFN) fabricated by a solid-phase method is studied. Before sintering, a synthesized PFN powder is processed in Bridgman anvils via a force action in combination with shear deformation (FASD) at room temperature. The electrophysical properties and structural parameters of processed samples and a reference sample are compared. Point defects are shown to play a key role in the formation of the physical properties beginning from an FASD of 200 MPa.