7 March 2018 in Materials Research Letters
Heteroepitaxial films of Ga O were grown on c-plane sapphire (0001). The stable phase β-Ga O was grown using the metalorganic chemical vapor deposition technique, regardless of precursor flow rates, at temperatures between 500 C and 850 C. Metastable α- and ϵ-phases were grown when using the halide vapor phase epitaxy (HVPE) technique, at growth temperatures between 650 C and 850 C, both separately and in combination. XTEM revealed the better lattice-matched α-phase growing semi-coherently on the substrate, followed by ϵ-Ga O . The epitaxial relationship was determined to be [ ] ϵ-Ga O [ ] α-Ga O [ ] α-Al O . SIMS revealed that epilayers forming the ϵ-phase contain higher concentrations of Cl introduced during HVPE growth. GRAPHICAL ABSTRACT IMPACT STATEMENT This study demonstrates one of the first epitaxial growths of multiple polymorphs of Ga O on sapphire (0001) substrates, including its β-, α-, and ϵ-phases. Epitaxial relationship is confirmed through HRTEM.
12 September 2016 in The Journal of Physical Chemistry Letters
15 January 2012 in Journal of Applied Physics
Carrier dynamics in hydride vapor phase epitaxy grown bulk GaN with very low density of dislocations, 5–8 × 105 cm−2, have been investigated by time-resolved photoluminescence (PL), free carrier absorption, and light-induced transient grating techniques in the carrier density range of 1015 to ∼1019 cm−3 under single and two photon excitation. For two-photon carrier injection to the bulk (527 nm excitation), diffusivity dependence on the excess carrier density revealed a transfer from minority to ambipolar carrier transport with the ambipolar diffusion coefficient Da saturating at 1.6 cm2/s at room temperature. An extremely long lifetime value of 40 ns, corresponding to an ambipolar diffusion length of 2.5 μm, was measured at 300 K. A nearly linear increase of carrier lifetime with temperature in the 80–800 K range and gradual decrease of D pointed out a prevailing mechanism of diffusion-governed nonradiative recombination due to carrier diffusive flow to plausibly the grain boundaries. Under single photon excitation (266 and 351 nm), subnanosecond transients of PL decay and their numerical modeling revealed fast processes of vertical carrier diffusion, surface recombination, and reabsorption of emission, which mask access to pure radiative decay.
9 January 2017 in IEEE Photonics Technology Letters
Free-standing nonpolar GaN substrates provide an excellent platform for the fabrication of high-speed blue and green light-emitting diodes (LEDs), which are attractive for visible-light communication, plastic optical fiber communication, and short-range under water optical communication. Nonpolar LEDs on free-standing GaN exhibit a large electron-hole wave function overlap, low extended defect density, and favorable thermal properties. Here, we demonstrate high-speed nonpolar InGaN/GaN LEDs with a peak emission wavelength between 455 and 465 nm on free-standing nonpolar GaN substrates. A large frequency modulation bandwidth of 524 MHz is demonstrated at a current density of 10 kA/cm 2 .
6 March 2018 in Crystal Growth & Design
2 December 2016 in Nanotechnology
ARAshwin K Rishinaramangalam
Ashwin K Rishinaramangalam
+1
Controlled bottom-up selective-area epitaxy (SAE) is used to tailor the morphology and photoluminescence properties of GaN/InGaN core–shell nanowire arrays. The nanowires are grown on c -plane sapphire substrates using pulsed-mode metal organic chemical vapor deposition. By varying the dielectric mask configuration and growth conditions, we achieve GaN nanowire cores with diameters ranging from 80 to 700 nm that exhibit various degrees of polar, semipolar, and nonpolar faceting. A single InGaN quantum well (QW) and GaN barrier shell is also grown on the GaN nanowire cores and micro-photoluminescence is obtained and analyzed for a variety of nanowire dimensions, array pitch spacings, and aperture diameters. By increasing the nanowire pitch spacing on the same growth wafer, the emission wavelength redshifts from 440 to 520 nm, while increasing the aperture diameter results in a ∼35 nm blueshift. The thickness of one QW/barrier period as a function of pitch and aperture diameter is inferred using scanning electron microscopy, with larger pitches showing significantly thicker QWs. Significant increases in indium composition were predicted for larger pitches and smaller aperture diameters. The results are interpreted in terms of local growth conditions and adatom capture radius around the nanowires. This work provides significant insight into the effects of mask configuration and growth conditions on the nanowire properties and is applicable to the engineering of monolithic multi-color nanowire LEDs on a single chip.